Patents
US 8,551,370 B2#61311722 Most CitedActiveUnited States (USPTO)Utility

Oxide sintered body, manufacturing method therefor, manufacturing method for transparent conductive film using the same, and resultant transparent conductive film

1Forward Citations (#61311722 Global)
0.1/yrCitation Velocity (#49631897 Global)
0.75Citation PageRank (#61311722 Global)
19Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An oxide sintered body substantially containing zinc, tin and oxygen; containing tin at an atomic number ratio, Sn/(Zn+Sn), of 0.23 to 0.50, and being composed mainly of a zinc oxide phase and at least one kind of zinc stannate compound phase, or being composed of at least one kind of zinc stannate compound phase; provided by a method for manufacturing the oxide sintered body by formulating an aqueous solvent to raw material powder containing powder of a zinc stannate compound, or mixed powder of tin oxide powder and zinc oxide powder, and after mixing the resulting slurry for equal to longer than 15 hours, by subjecting the slurry to solid-liquid separation, drying and granulation and subsequently compacting by charging the granule into a mold followed by sintering the resultant compact under sintering atmosphere at 1300 to 1500° C. for equal to or longer than 15 hours.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An oxide sintered body consisting essentially of zinc, tin and oxygen, characterized by containing tin at an atomic number ratio, Sn/(Zn+Sn), of 0.23 to 0.50, and wherein the oxide sintered body contains a zinc stannate compound, wherein the zinc stannate compound includes at least one selected from the group consisting of Zn 2 SnO 4 having a tin element as solid solution at the Zn site thereof, and Zn 2 SnO 4 with a non-stoichiometric composition having a ratio of Sn/(Zn+Sn) that is a little deviated from that of Zn 2 SnO 4 , and wherein the oxide sintered body does not contain a detectable

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
US 4,716,086 AProtective overcoat for low emissivity coated article1987193
JP H02145458 ALowly reflective, densely colored coated article and its manufacture—3
JP H02149459 AOxide sintered body, production and use thereof—49
JP H08171824 AManufacture of transparent conductive film—32
JP 2000207935 ATransparent conductive material, transparent conductive glass and tranparent conductive film—12
JP 2000256061 ATransparent conductive material, transparent conductive glass and transparent conductive film—59
CN 1,369,572 AElectrically conducting transparent oxide film—22
US 6,534,183 B1Target for transparent electroconductive film, transparent electroconductive material, transparent electroconductive glass, and transparent electroconductive film200362
US 2003148871 A1Target for transparent electroconductive film, transparent electroconductive material, transparent electroconductive glass and transparent electroconductive film—34
US 6,669,830 B1Sputtering target, transparent conductive oxide, and process for producing the sputtering target200388
US 6,899,953 B1Shippable heat-treatable sputter coated article and zinc cathode sputtering target containing low amounts of tin200555
JP 2005154820 ASputtering target, and optical information recording medium, and method for manufacturing the same—21
JP 2006169200 AMethod for screening insulin secretion promoting agent—3
JP 2006194926 AMethod for manufacturing transparent electrode—15
JP 2006196201 AClear electrode and its manufacturing method—7
JP 2007031786 ASputtering target, manufacturing method therefor and transparent electroconductive film—18
JP 2007314364 AOxide sintered compact, target, oxide transparent conductive film obtained by using the same and method of manufacturing the same—44
US 2009308635 A1Sputtering target, transparent conductive film, and transparent electrode for touch panel—39
US 2010170696 A1Sputtering target, transparent conductive film and transparent electrode—57

Non-Patent Literature (5)

  • "Transparent conductive film technology," Japan Society for the Promotion of Science; Ohmsha, Ltd., 1999, pp. 125 and 173, including cover sheet, table of contents and end sheet (6 Sheets total).
  • Abboudy et al., "Influence of substrate temperature on the electrical behaviour of zinc stannate thin films . . . ", II Nuovo Cimento 20D, No. 12, Dec. 1998, 1881-90.
  • Al-Shahrani et al., "Absence of the Coulomb gap at the Femi level in the variable range hopping regime of zinc stannate polycrystalline systems", J Phys D: Appl Phys 29, (1996), 2165-69.
  • European Search Report dated Nov. 4, 2010.
  • H. Enoki et al., "The Electrical and Optical Properties of the ZnO-SnO2 Thin Films Prepared by RF Magnetron Sputtering", Phys. Stat. Sol. (a) 129, 181 (1992). p. 181, XP009036246.