Preparation of metal colloids
Abstract
A method is described for producing a silver colloid solution comprised of highly stable resulting colloids, the method comprising: adding an aqueous solution of a hydroxylamine salt to an aqueous solution of an alkali, and then dispersing into the mixture an aqueous solution of the metal ions, the hydroxylamine salt being selected such that the anion, when combined with the said metal ions, would form a metal salt having a very low solubility in water, wherein the metal ion solution is introduced into the mixture in such a manner that the metal ions are substantially dispersed throughout the mixture within one second. A maturing period, preferably at elevated temperatures, leads to a stable state in which the characteristics of the colloid undergo no further changes, and it is preferred to make and store the colloid in a polystyrene container for greatest stability. The resulting colloids from such method exhibit high light-scattering properties of small particle size and low background fluorescence levels, with a long shelf life, making it particularly suitable for Raman spectroscopy.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing a metal colloid solution, comprising adding an aqueous solution of a hydroxylamine salt to an aqueous solution of an alkali, and then introducing into the mixture an aqueous solution of the metal ions, the hydroxylamine salt being selected such that the anion, when combined with the said metal ions, would form a metal salt having a solubility product (K sp ) value of less than 1×10 −10 in water, wherein the metal ion solution is introduced into the mixture in such a manner that the metal ions are substantially dispersed throughout the mixture within one second.
- Claim 2Depends on #1
A method according to claim 1 , wherein the metal ions are introduces into and mixed with the mixture within 0.5 second.
- Claim 3Depends on #1
A method according to claim 1 , wherein the metal is silver.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 9,086,381 B2 | Preparation of metal colloids | 2015 | 0 |
| US 2014124707 A1 | Preparation of Metal Colloids | — | 0 |
References Cited — Backward Prior Art (6)
Non-Patent Literature (2)
- http://www.merriam-webster.com/thesaurus/predominantly General knowledge, from the world wide web on Jan. 24, 2013.
- Nitrate Wtih Hydroxylamine Hydrochloride, J. Phys. Chem B., vol. 107, No. 24, May 22, 2003, pp. 5723-5727, XP002527546, cited in the application, pp. 5724-5726.