Method and apparatus for enhanced size reduction of particles
Abstract
The present invention provides methods and apparatus for producing particles via supercritical fluid processing. In one embodiment, the method includes expanding a supercritical fluid plasticized melt across a pressure drop to form solid composite particles that are simultaneously dispersed, foamed and cooled, and milling the solid particles produced to achieve the desired size distribution. In another embodiment, a pressure vessel containing a supercritical fluid plasticized melt is depressurized to form a cooled solid porous mass, which is then milled to obtain solid composite particles.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing solid particles comprising the steps of: providing a load stock comprising: an excipient that is a solid at 25° C. and 1 atmosphere pressure; and optionally, a biologically active substance; contacting the load stock with a supercritical fluid in a pressure vessel that is pressurized and heated to maintain said fluid supercritical, and to form a melt; depressurizing the pressure vessel to transform the melt in the pressure vessel into a solid porous mass that is cooled to a temperature below 25° C.; and milling the solid porous mass to obtain solid particles.
- Claim 2Depends on #1
The method according to claim 1 wherein the solid porous mass is milled before the temperature of the solid porous mass is permitted to rise to 25° C.
- Claim 3Depends on #1
The method according to claim 1 wherein subsequent to the mi
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (12)
Non-Patent Literature (3)
- Chattopadhyay, P. and Gupta, R., Production of Antibiotic Nanoparticles Using Supercritical CO2 as Antisolvent with Enhanced Mass Transfer, Ind. Eng. Chem. Res., 2001, vol. 40, pp. 3530-3539.
- Chattopadhyay, P. and Gupta, R., Protein Nanoparticles Formation by Supercritical Antisolvent with Enhanced Mass Transfer, AIChE Journal, Feb. 2002, vol. 48, No. 2, pp. 235-244.
- Supplementary European Search Report for corresponding EP 04809300.0 mailed Jan. 5, 2012, three pages.