Abstract

The invention provides a deep groove ball bearing which exhibits a long life even in a high-temperature environment or an environment involving the penetration of water in spite of its low alloying element content. The outer race, inner race and ball constituting the bearing are made of a steel which contains 0.3 to 0.4% of carbon, 0.3 to 0.7% of silicon, 0.3 to 0.8% of manganese, 0.5 to 1.2% of nickel, 1.6 to 2.5% of chromium, 0.1 to 0.7% of molybdenum and 0.2 to 0.4 of vanadium with the balance consisting of iron and impurities and in a total content of silicon and manganese of 1.0% or below, a total content of nickel and chromium of 2.3% or above and a total content of chromium, molybdenum and vanadium of 3.0% or below. Surface hardened layers are formed in the outer race, inner race and ball respectively and the surface hardened layers exhibit hardness of 725 to 800 HV, while the maximum particle size of carbides dispersed in the surface hardened layers is 10 μm or below and the area ratio thereof is 7 to 25%. Further, the inner parts exhibit hardness of 450 to 650 HV.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 46 · Forward citations: 9.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A rolling member constituted of steel containing at least 0.3 mass % and not more than 0.4 mass % of carbon, at least 0.3 mass % and not more than 0.7 mass % of silicon, at least 0.3 mass % and not more than 0.8 mass % of manganese, at least 0.5 mass % and not more than 1.2 mass % of nickel, at least 1.6 mass % and not more than 2.5 mass % of chromium, at least 0.1 mass % and not more than 0.7 mass % of molybdenum and at least 0.2 mass % and not more than 0.4 mass % of vanadium, and a balance of the steel is iron and impurities, in which the sum of the content of silicon and the content of man

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Decision to Grant Patent issued in Japanese Patent Application No. 2007-153136 dated Apr. 2, 2013.
  • Decision to Grant Patent issued in Japanese Patent Application No. 2007-156703 dated Apr. 2, 2013.
  • English Abstract and English Machine Translation of Fujita (JP 2005-314794) (2005).
  • Office Action issued in Japanese Application No. 2007-153136 dated Jan. 8, 2013.