Abstract

A photosensitive glass paste that can be fired at a low temperature for a short period of time and that can suppress generation of voids and diffusion of Ag in glass layers formed by firing, and a high-performance multilayer wiring chip component manufactured by using the above photosensitive glass paste are provided. As a sintering aid glass which is combined with a ceramic aggregate and a primary glass, a glass having a contact angle to the ceramic aggregate smaller than that of the primary glass to the ceramic aggregate is used, and the content of the sintering aid glass is set to 5 to 10 percent by volume of the inorganic component. As the sintering aid glass, a glass containing SiO 2 , B 2 O 3 , CaO, Li 2 O, and ZnO at a predetermined ratio is preferably used. As the primary glass, a glass containing 70 to 90 percent by weight of SiO 2 , 15 to 20 percent by weight of B 2 O 3 , and 1 to 5 percent by weight of K 2 O can be used.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A photosensitive glass paste adapted to form glass layers by firing when a multilayer wiring chip component is manufactured that includes the glass layers and at least one conductor layer formed between a pair of glass layers by firing a photosensitive Ag paste, the photosensitive glass paste comprising: an inorganic component comprising a primary glass, a sintering aid glass, and a ceramic aggregate; and a photosensitive organic component, wherein the softening point of the sintering aid glass is 609° C. or more and the sintering glass has a content of SiO 2 of 45 to 60 percent by weight, th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
JP H03150141 AManufacture of double-toothed belt—2
JP H0818236 AMethod for manufacturing layered ceramic circuit board—6
JP H1087342 ANonmagnetic ceramic and ceramic laminated part—3
JP H10289822 AElectronic component and wafer—7
JP H11204336 AProduction of high-frequency inductor—8
US 6,117,614 APhotosensitive glass paste200017
JP 2000275826 APaste composition and circuit board using same—9
US 6,183,669 B1Paste composition, circuit board using the same, ceramic green sheet, ceramic substrate, and method for manufacturing ceramic multilayer substrate200152
JP 2001114554 ALow-temperature burnable ceramic composition and ceramic multilayer substrate—9
JP 2001210141 AMethod of manufacturing photosensitive glass plate and multilayer wiring circuit board using it—17
US 2001014429 A1Photosensitive glass paste and method for manufacturing multilayered interconnected circuit board using the same—12
US 2002001881 A1Glass and glass tube for encapsulating semiconductors—13
JP 2002037641 AGlass for encapsulation of semiconductor, external cylinder for semiconductor encapsulation and method of encapsulation of semiconductor element—31
US 6,365,265 B1Photosensitive insulating paste and thick-film multi-layer circuit substrate200213
US 6,455,453 B1Low-temperature sinterable ceramic composition and multilayer ceramic substrate200221
JP 2003104755 APaste—18
US 2003203317 A1Photosensitive glass paste and method for manufacturing multilayered interconnected circuit board using the same—3
US 7,146,719 B2Multilayer circuit component and method for manufacturing the same20064

Non-Patent Literature (1)

  • International Search Report issued for International Application PCT/JP2008/051292 dated Mar. 18, 2008.