US 8,524,512 B2#60821703 Most CitedActiveUnited States (USPTO)Utility

Method for repairing copper diffusion barrier layers on a semiconductor solid substrate and repair kit for implementing this method

1Forward Citations (#60821703 Global)
0.1/yrCitation Velocity (#49596421 Global)
0.76Citation PageRank (#60821703 Global)
14Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Method for repairing copper diffusion barrier layers on a semiconductor solid substrate and repair kit for implementing this method. One subject of the present invention is a method for repairing a surface of a substrate coated with a discontinuous copper diffusion barrier layer of a titanium-based material. According to the invention, this method comprises: a) the contacting of the surface with a suspension containing copper or copper alloy nanoparticles for a time of between 1 s and 15 min; and b) the contacting of the thus treated surface with a liquid solution having a pH of between 8.5 and 12 and containing: at least one metal salt, at least one reducing agent, at least one stabilizer at a temperature of between 50° C. and 90° C., preferably between 60° C. and 80° C., for a time of between 30 s and 10 min, preferably between 1 min and 5 min, in order to thus form a metallic film having a thickness of at least 50 nanometers re-establishing the continuity of the copper diffusion barrier layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for repairing a surface of a substrate, said substrate being coated with a discontinuous copper diffusion barrier layer of a titanium-based material defining said surface to be repaired, which comprises: a) contacting said surface with a suspension containing copper or copper alloy nanoparticles for a time of between 1 s and 15 min, thus causing the nanoparticles to be selectively adsorbed onto the surface of the barrier layer; and b) contacting the thus treated surface with a liquid solution having a pH of between 8.5 and 12 and comprising: at least one metal salt, at least one reduc

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Lo et al., "Long-term stability of Cu/Pd nanoparticles and their feasibility for electroless copper deposition," Electrochimica Acta, Elsevier Science Publishers, vol. 54, No. 2, pp. 727-732, 2008.
  • Topol et al., "Three-dimensional integrated circuits," IBM J. Res. & Dev., vol. 50, No. 4/5, pp. 491-506, 2006.