Patents
US 8,524,093 B2#34719839 Most CitedActiveUnited States (USPTO)Utility

Method for forming a deep trench

2Forward Citations (#34719839 Global)
0.1/yrCitation Velocity (#38437889 Global)
1.56Citation PageRank (#21519086 Global)
9Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for forming a deep trench includes providing a substrate with a bottom layer and a top layer; performing a first etching process to etch the top layer, the bottom layer and the substrate so as to form a recess; selectively depositing a liner covering the top layer, the bottom layer and part of the substrate in the recess; using the liner as an etching mask to perform a second dry etching to etch the recess unmasked by the liner so as to form a deep trench; performing a selective wet etching to remove the top layer; and performing a post wet etching to enlarge the deep trench.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming a deep trench, comprising the steps of: providing a substrate having a pad layer formed on a top face of the substrate, wherein the pad layer comprises a first layer of a combination of oxide and nitride and a second layer of silicate glass, and the second layer is on a top surface of the first layer; performing a first etching process to form a first trench through the pad layer and into the substrate, wherein the first trench includes a sidewall and a bottom surface; after the first etching process, forming a liner to cover a top surface of the pad layer and the sidewall

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗