Decolorization of polyols
Abstract
Natural oil-based polyols that are high in color, e.g., >40 APHA, are decolorized when exposed to high frequency visible light and/or low frequency UV light, with or without the combination of heat and/or air exposure.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for decolorizing a natural oil-based polyol, the process comprising the step of exposing the polyol to actinic radiation of a wavelength of 250 to 550 nanometers.
- Claim 2Depends on #1
The process of claim 1 in which the polyol is exposed to the actinic radiation at a temperature between ambient and 120 ° C.
- Claim 3Depends on #2
The process of claim 2 in which the polyol is simultaneously contacted with an oxygen source.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (13)
Non-Patent Literature (1)
- International Search Report and Written Opinion mailed Feb. 22, 2011 for PCT App. No. PCT/US2010/056672.