Patents
US 8,518,530 B2#118643180 Most CitedActiveUnited States (USPTO)Utility

Production method for an ultra-low-dielectric-constant film, and an ultra-low-dielectric-constant film produced thereby

0Forward Citations (#118643180 Global)
0.0/yrCitation Velocity (#118643180 Global)
0.56Citation PageRank (#118643180 Global)
15Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a production method for an ultra-low-dielectric-constant film, in which ratios are optimised in a mixed solution having a matrix consisting of a poly (alkyl silsesquioxane) copolymer and a porogen represented by Chemical formula 1, and in which this mixed solution is subjected to ultraviolet curing during a heat treatment. The ultra-low-dieletric-constant film of the present invention can be used as an intermediate insulating film for next generation semiconductors instead of the SiO2 dielectric films currently used, since pores of from 1 to 3 nm are uniformly distributed at from 10 to 30% and a very high degree of mechanical elasticity of from 10.5 to 19 GPa is achieved at a low dielectric constant from 2.12 to 2.4.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of preparing an ultralow dielectric film, comprising: putting a compound represented by the following Formula 1 and a poly alkyl silsesquioxane copolymer into an organic solvent to prepare a mixed solution and then coating the mixed solution on a substrate to form a thin film; heating the thin film to 200 to 300° C.; and subjecting the thin film to heat treatment after raising the thin film to 350 to 500° C. and irradiating an ultraviolet (UV) ray at a wavelength of 200 to 300 nm onto the thin film for 5 to 30 min during the heat treatment: R 1 OCH 2 [CH(OR 2 )] n CH 2 OR 3   [Formula

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (15)

PatentTitleYearCitations
US 6,271,273 B1Porous materials2001166
US 6,451,712 B1Method for forming a porous dielectric material layer in a semiconductor device and device formed2002120
KR 20020079075 Apoly(methyldilsesquioxane)copolymers, low-dielectric films therefrom and preparation method thereof—3
US 2004109950 A1Dielectric materials—39
KR 100,455,339 B1Composition for preparing materials having nano-porosity20044
KR 100,508,696 B1Ultra-low Dielectrics for Copper Interconnect20052
US 2006014845 A1Low dielectric organosilicate polymer composite—5
KR 100,589,123 B1Cyclodextrin Derivatives as Pore-forming Templates, and Low Dielectric Material Prepared by Using It20066
US 2006142504 A1Novel polymer and production of nano-porous low dielectric polymer composite film using the same—16
KR 100,595,526 B1Ultra-low Dielectrics Prepared by Monosaccharide Derivatives for Cupper Interconnect20067
KR 100,672,905 B1Reactive Porogen Based on Organic Noncyclic-polyol, and Ultra-low Dielectric Materials Prepared by Using It20076
US 7,169,477 B2Composition for preparing porous dielectric thin films20077
US 2009146265 A1ULTRA LOW k PLASMA ENHANCED CHEMICAL VAPOR DEPOSITION PROCESSES USING A SINGLE BIFUNCTIONAL PRECURSOR CONTAINING BOTH A SiCOH MATRIX FUNCTIONALITY AND ORGANIC POROGEN FUNCTIONALITY—5
US 2011101489 A1SiCOH DIELECTRIC MATERIAL WITH IMPROVED TOUGHNESS AND IMPROVED Si-C BONDING, SEMICONDUCTOR DEVICE CONTAINING THE SAME, AND METHOD TO MAKE THE SAME—7
US 2012328796 A1Materials containing voids with void size controlled on the nanometer scale—6

Non-Patent Literature (1)

  • The International Search Report dated Oct. 18, 2010.