Abstract

An Ni-Fe based superalloy forging material including 30 to 40 wt % of Fe, 14 to 16 wt % of Cr, 1.2 to 1.7 wt % of Ti, 1.1 to 1.5 wt % of Al, 1.9 to 2.2 wt % of Nb, 0.05 wt % or less of C and the remainder of Ni and inevitable impurities is solution-treated and aged, and thereby gamma' phase (Ni3Al) having an initial mean particle size of about 50 to about 100 nm is precipitated. This superalloy is excellent in high-temperature strength and high-temperature ductility and can produce a large forged product of 10 ton or more. Therefore, this material is suitable for use as the material of a steam turbine rotor having a main steam temperature of 650° C. or more.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 3.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An Ni—Fe based forging superalloy comprising 30 to 40 wt % of Fe, 14 to 16 wt % of Cr, 1.2 to 1.7 wt % of Ti, 1.1 to 1.5 wt % of Al, 1.9 to 2.2 wt % of Nb, 0.05 wt % or less of C, and the remainder of Ni and inevitable impurities, wherein γ′ phase (Ni 3 Al) precipitate having an initial mean particle size of 50 to 100 nm is enhanced in the grain, wherein said Ni—Fe based superalloy forging material has a 0.2% yield strength of 450 to 600 MPa at 700° C. and reduction of area of 25% or greater, and wherein the C is bonded with Nb and Ti to form MC carbide.

  2. Claim 2Independent Claim

    A steam turbine rotor formed of an Ni—Fe based superalloy forging material comprising 30 to 40 wt % of Fe, 14 to 16 wt % of Cr, 1.2 to 1.7 wt % of Ti, 1.1 to 1.5 wt % of Al, 1.9 to 2.2 wt % of Nb, 0.05 wt % or less of C, and the remainder of Ni and inevitable impurities, wherein

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • ASM International, Materials Park, Ohio, ASM Specialty Handbook: Nickel, Cobalt, and Their Alloys: "Metallography, Microstructures, and Phase Diagrams of Nickel and Nickel Alloys", Dec. 2000, vol. 2, pp. 302-304.
  • European Search Report, EP 07015815, Nov. 22, 2007, 5 pp.
  • Imano, Shinya et al, "Modification of Alloy 706 for High Temperature Steam Turbine Rotor Application", Superalloy 718, 625, 706 and Various Derivatives TMS, 2005, pp. 77-86.