Patents
US 8,512,422 B2#28748592 Most CitedActiveUnited States (USPTO)Utility

Solid electrolytic capacitor containing an improved manganese oxide electrolyte

3Forward Citations (#28748592 Global)
0.2/yrCitation Velocity (#30824020 Global)
1.43Citation PageRank (#24656603 Global)
26Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A solid electrolytic capacitor that contains an anode body formed from an electrically conductive powder and a dielectric coating located over and/or within the anode body is provided. The powder has a high specific charge and in turn a relative dense packing configuration. Despite being formed from such a powder, the present inventors have discovered that a manganese precursor solution (e.g., manganese nitrate) can be readily impregnated into the pores of the anode. This is accomplished, in part, through the use of a dispersant in the precursor solution that helps minimize the likelihood that the manganese oxide precursor will form droplets upon contacting the surface of the dielectric. Instead, the precursor solution can be better dispersed so that the resulting manganese oxide has a “film-like” configuration and coats at least a portion of the anode in a substantially uniform manner. This improves the quality of the resulting oxide as well as its surface coverage, and thereby enhances the electrical performance of the capacitor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming a solid electrolytic capacitor, the method comprising: anodically oxidizing an anode body to form a dielectric coating, wherein the anode body is formed from a powder; contacting the dielectric-coated anode body with a solution that contains a manganese oxide precursor and a dispersant; and pyrolytically converting the precursor to a manganese oxide solid electrolyte.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the dispersant contains an organic compound having a hydrophilic moiety and a hydrophobic moiety, which is an aromatic or heteroatomic ring system having from 6 to 14 carbon atoms.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the hydrophilic moiety includes a sulfonate, phosphonate, carboxylate, thiol, sulfonate ester, phosphite, phosphonite, phosphinite, phosphate, sulfate, phosphate ester, su

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (26)

PatentTitleYearCitations
US 3,067,243 APreparation of salts of naphthalene sulfonic acid-formaldehyde condensates196219
US 3,337,429 ASolid electrolytic capacitor and process therefor196720
US 3,627,694 AProduction of aqueous suspension of manganese dioxide19719
US 3,773,539 AMethod of preparing light-sensitive photographic material with manganese dioxide layer19736
US 4,042,420 AMethod of producing manganese oxide solid electrolyte capacitor197718
US 4,072,586 AManganese dioxide electrodes197827
US 4,184,192 ASolid electrolyte compacitor using low resistivity metal oxide as cathode collector198037
US 4,243,503 AMethod and electrode with admixed fillers198130
US 4,302,301 ASolid electrolyte deposition on anodized pellets198113
US 5,268,408 AProcess for the preparation of colloidal manganese dioxide19937
US 5,560,761 ATantalum powder and electrolytic capacitor using same199646
US 5,622,746 ATantalum capacitor impregnation process199726
US 5,629,830 ASolid state electrolytic capacitor having a concave199729
US 6,337,160 B1Manganese dioxide electrodes, process for producing the same and their use200219
US 6,336,944 B1Method of manufacturing solid electrolytic capacitors20023
US 6,377,443 B1Thermal treatment process for valve metal nitride electrolytic capacitors having manganese oxide cathodes200210
US 6,689,187 B2Tantalum powder for capacitors200422
US 6,849,134 B2Minimum volume oven for producing uniform pyrolytic oxide coatings on capacitor anodes20055
US 6,939,528 B2Manganese dioxide for alkaline cells20055
US 6,982,865 B2Solid electrolytic capacitor200615
GB 2,443,503 ACapacitor Assembly—7
GB 2,445,673 AA Fused Electrolytic Capacitor—10
GB 2,456,858 AElectrolytic Capacitor Anode Formation—5
GB 2,458,550 AElectrolytic Capacitor Assembly Containing a Resettable Fuse—7
US 2010302712 A1Solid Electrolytic Capacitor with Facedown Terminations—16
US 2011317334 A1Solid Electrolytic Capacitor for Use in High Voltage Applications—7

Non-Patent Literature (5)

  • Article-Dias et al., "On the performance of pyrolytic MnO2/tantalum capacitors: Columnar vs. nanocrystalline cathodic layers," Acta Materialia, vol. 55, Issue 11, Jun. 2007, pp. 3757-3763.
  • Article—Dias et al., "On the performance of pyrolytic MnO2/tantalum capacitors: Columnar vs. nanocrystalline cathodic layers," Acta Materialia, vol. 55, Issue 11, Jun. 2007, pp. 3757-3763.
  • Article-Kabir-ud-Din et al., "Effect of surfactants on the oxidation of oxalic acid by soluble colloidal MnO2," Colloids and Surfaces A: Physicochem. Eng. Aspects, vol. 234, 2004, pp. 159-164.
  • Article—Kabir-ud-Din et al., "Effect of surfactants on the oxidation of oxalic acid by soluble colloidal MnO2," Colloids and Surfaces A: Physicochem. Eng. Aspects, vol. 234, 2004, pp. 159-164.
  • Article-Perez-Benito et al., "A Kinetic Study of the Reaction between Soluble (Colloidal) Manganese Dioxide and Formic Acid," Journal of Colloid and Interface Science, vol. 149, No. 1, Mar. 1, 1992, pp. 92-97.