Water based slurry compositions for making environmental barrier coatings and environmental barrier coatings comprising the same
Abstract
Water based slurry compositions for making an environmental barrier coating including from about 1 wt % to about 99.9 wt % water; from about 0.1 wt % to about 72 wt % primary material; and from about 0.1 wt % to about 25 wt % slurry sintering aid.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 16.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A water based slurry composition adapted to be sintered to form an environmental barrier coating, the slurry composition comprising: from about 1 wt % to about 99.9 wt % water; from about 0.1 wt % to about 72 wt % of a primary material chosen from the group consisting of rare earth disilicates, doped rare earth disilicates, rare earth monosilicates, doped rare earth monosilicates, barium-strontium-aluminosilicates or rare earth doped barium-strontium-aluminosilicates; and from about 0.1 wt % to about 25 wt % of at least one slurry sintering aid that is reactive with the primary material to for
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗