Method for manufacturing basalt fiber
Abstract
Basalt filament is manufactured such that the fiber diameter can be controlled and the filament is not severed during winding. A network former and a glass modifier are formed and maintained with respect to basalt rock ore, and the crystallization and binding of basalt fiber are inhibited, the heat-resistance property of basalt fiber is greatly improved from the conventional 750° C. to 850 or 900° C., and significant cost reduction is achieved over conventional products. The method includes: grinding basalt rock as a material; washing a resultant ground rock; melting the ground rock that has been washed; transforming a molten product into fiber; and drawing the fiber in an aligned manner, and winding it. The temperature of the molten product in the melting step is 1400 to 1650° C., and log η is 2.15 to 2.35 dPa·s and preferably 2.2 to 2.3 dPa·s, where η is the viscosity of the molten product.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 37 · Forward citations: 5.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Basalt filament manufactured by a method for manufacturing, comprising the steps of: grinding basalt rock material; washing a resultant ground rock; melting the ground rock that has been washed; transforming a molten product into fiber; and drawing the fiber in an aligned manner, and winding it to produce the basalt filament, wherein the temperature of the molten product in the melting step is 1400 to 1650° C., and wherein log η is 2.15 to 2.35 dPa·s, where η is the viscosity of the molten product, wherein the basalt rock material comprises a mixture of 85 wt % of a high-temperature basalt roc
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (37)
Non-Patent Literature (5)
- Chinese Office Action issued May 8, 2009 for Application No. 2006100930453.
- Communication and European Search Report for European Application No. EP 06253154.6-2122, mailed Sep. 28, 2006 (4 pages).
- First Examination Report for Korean Patent Application No. 10-2006-0055086 dated Mar. 27, 2007 (3 pages).
- Fyodorovich et al., "Method of Inorganic Fibers Production from Rocks," Ukrainian patent No. UA (11) 10672 (13) A-Published Dec. 25, 1996.
- Grigor'jevna et al., "Method for basalt Fiber Production and Device for its Accomplishment," Russian Patent No. RU(11)2118300(13) C1-Published Nov. 19, 1998.