Patents
US 8,501,146 B2#61585723 Most CitedActiveUnited States (USPTO)Utility

Preparation method for hollow carbon fiber using supercritical fluid

1Forward Citations (#61585723 Global)
0.1/yrCitation Velocity (#49653582 Global)
0.75Citation PageRank (#61585723 Global)
9Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Disclosed is a method for preparing hollow carbon fibers having an empty space in the cross section thereof. More specifically, the disclosed method includes melt-spinning an acrylonitrile-based polymer by using a supercritical fluid as a plasticizer; drawing spun fibers to prepare hollow precursor fibers; and stabilizing and carbonizing the hollow precursor fibers to prepare the hollow carbon fibers. The hollow carbon fibers obtained by the disclosed method have at least a 10 to 50% lower specific gravity than conventional hollow carbon fibers (solid), but have similar mechanical properties to the conventional fibers. Furthermore, the diameter of carbon fibers can be adjusted, thereby making it possible to widen the application of hollow carbon fibers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for preparing hollow carbon fibers, the method comprising: melt-spinning an acrylonitrile-based polymer having a weight average molecular weight ranging from 200,000 to 500,000 g/mol by using a supercritical fluid as a plasticizer; drawing spun fibers to prepare hollow precursor fibers; and stabilizing and carbonizing the hollow precursor fibers to prepare the hollow carbon fibers, wherein a spinneret used for the melt-spinning has a hollow outer diameter ranging from 0.2 to 0.3 mm, a hollow inner diameter ranging from 0.07 to 0.17 mm, and a spinneret interval ranging from 0.01 to 0.1

  2. Claim 2Depends on #1

    The method as claimed in claim 1 , wherein the acrylonitrile-based polymer comprises acrylonitrile units in an amount of 90 wt % or more with respect to a total polymer weight.

  3. Claim 3Independent Claim

    The method as claimed in c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • Baird et al.; Absorption of Carbon Dioxide and Subsequent Viscosity Reduction of an Acrylonitrile Copolymer; Polymer; 45, pp. 3399-3412; 2004.
  • Hu et al.; Molecular Weight Distribution of Polyacrylonitrile Produced in Supercritical Carbon Dioxide; Journal of Applied Polymer Science; vol. 86, issue 9, pp. 2338-2341; Sep. 18, 2002.
  • Ismail et al.; Post Spinning and Pyrolysis Processes of Polyacrylonitrile (PAN)-based Carbon Fiber and Activated Carbon Fiber; A Review; Journal of Analytical and Applied Pyrolysis; 91, pp. 1-13; Oct. 15, 2011.