Patents
US 8,501,071 B2#18722415 Most CitedActiveUnited States (USPTO)Utility

Method for obtaining high-tenacity aramid yarn

6Forward Citations (#18722415 Global)
0.5/yrCitation Velocity (#17840725 Global)
1.31Citation PageRank (#28095935 Global)
21Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a method for obtaining high-tenacity aramid yarn, wherein the yarn is made of a copolymer obtained from a mixture of monomers comprising DAPBI, an aromatic para-diamine, and an aromatic para-diacid, wherein the yarn is heated in at least two process steps, characterized in that in a first step the yarn is heated at a temperature of 200 to 360° C. at a tension of at least 0.2 cN/dtex, followed by a second step wherein the yarn is heated at a temperature of 370 to 500° C. at a tension of less than 1 cN/dtex. The invention further pertains to a multifilament aramid yarn spun from a sulfuric acid spin dope and having a tenacity of at least 2500 mN/tex.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for obtaining high-tenacity aramid yarn, wherein the yarn has a tenacity of at least 2750 mN/tex and is made of a copolymer obtained from a mixture of monomers comprising at least 12.5 mole% DAPBI, an aromatic para-diamine, and an aromatic para-diacid, and the yarn is heated in at least two process steps, the process steps comprising: a first step where the yarn is heated at a temperature of 200to 360° C. at a tension of at least 0.2cN/dtex, followed by a second step where the yarn is heated at a temperature of 370to 500° C. at a tension of less than 1 cN/dtex, wherein the tension in

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the yarn after the first process step is directly led to a heating device for performing the second process step without

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 3,227,793 ASpinning of a poly(polymethylene) terephthalamide1966191
US 3,414,645 AProcess for spinning wholly aromatic polyamide fibers1968264
US 3,767,756 ADry jet wet spinning process1973547
US 3,869,429 AHigh strength polyamide fibers and films1975487
US 4,018,735 AAnisotropic dopes of aromatic polyamides1977118
US 4,172,938 AProcess for producing polyamides with lactam or urea solvent and CaCl21979235
US 4,883,634 AProcess for manufacturing a high modulus poly-p-phenylene terephthalamide fiber19896
US 5,175,239 AProcess for making para-aramid fibers having high tenacity and modulus by microwave annealing199223
RU 2,017,866 C1Molded article199434
RU 2,045,586 C1Anisotropic solution for molding thread and thread which is prepared of said solution199586
US 5,571,891 AAromatic copolyamides, production thereof, formed structures and production thereof199685
US 5,646,234 AProduction of fibers or films using specific forming solutions and the fibers of films obtainable thereby199751
US 5,667,743 AWet spinning process for aramid polymer containing salts1997240
CN 1,473,969 APost-treatment new process for aramid fibre III raw tow—19
WO 2005/054337 A1Process for making dapbi-containing aramid crumbs—88
WO 2006/045517 A1Method for dissolving ppta in sulfuric acid using a twin screw extruder—7
RU 2,285,761 C1Method of manufacturing high-strength heat-resistant threads from aromatic copolyamide having heterocycles in the chain200629
US 2007083032 A1Process for making dapbi-containing aramid crumbs—34
WO 2008/061668 A1Method for obtaining high-tenacity aramid yarn—80
US 2010029159 A1Heterocycle-containing aromatic polyamide fiber, method for producing the same, cloth constituted by the fiber, and fiber-reinforced composite material reinforced with the fiber—97
US 2013075950 A1Copolymer fibers and yarns and processes for making same—4

Non-Patent Literature (5)

  • A.N. Gladkov et al., "Chemistry and Technology of Chemical Fibres," Fibre Chemistry, vol. 36, No. 3, pp. 177-180, 2004.
  • J.W.S. Hearle, High-Performance Fibres, 2004, cover pages (5) and pp. 115-118.
  • Sugak et al., "Fabrication of Fibres from Sulfuric Acid Solutions of Copolyamides Containing Polyamide-Benzimidazole Units and their Heat Treatment," Fibre Chemistry, vol. 31, No. 1, 1999, pp. 8-13.
  • V.N. Sugak et al., "Fabrication of Fibres From Sulfuric Acid Solutions of Copolyamides Containing Polyamide-Benzimidazole Units and Their Heat Treatment," Fibre Chemistry, vol. 31, No. 1, pp. 8-13, 1999.
  • Yang, Kevlar Aramid Fiber, 1992, pp. 34-35.