Patents
US 8,496,901 B2#60574511 Most CitedActiveUnited States (USPTO)Utility

Preparation method for a water-insoluble crystal form II ammonium polyphosphate with high purity and polymerization degrees

1Forward Citations (#60574511 Global)
0.1/yrCitation Velocity (#49580060 Global)
0.76Citation PageRank (#60574511 Global)
3Prior Art Cited
3Claims (3 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A preparation method for a water-insoluble crystal form ammonium polyphosphate includes conveying crystal H-type phosphorus pentoxide and diammonium phosphate at a molar ratio of 1:1-1.5 into a malaxator with twin screws, and injecting ammonia gas for 3-40 minutes into the malaxator at 20-25 m 3 /h while preheating the material at a temperature between 100° C. and 300° C. Therafter one injects ammonia gas again at 8-15 m 3 /h for 4-8 hours. The resulting material is transferred to another sealed container and stirred while coupling agent is added. Stirring continues until the material drops below 60° C., the material then being transferred into organic solvent for washing for 30-50 minutes. Thereafter the material is first filter pressed, then subjected to low temperature drying, and then sieved to obtain the final product.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 1.

Claims (3 — 3 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    conveying crystal H-type phosphorus pentoxide and diammonium phosphate at a molar ratio of 1:1-1.5 into a malaxator with twin screw, and injecting ammonia gas into the malaxator at 20-25 m 3 /h while preheating the phosphorus pentoxide and diammonium phosphate in the malaxator at a temperature between 100° C. and 300° C.;

  2. Claim 2Independent Claim

    after injecting ammonia gas for 30-40 minutes, stopping to add ammonia supplying compound to the malaxator, and then injecting ammonia gas into the malaxator again at 8-15 m 3 /h for 4-8 hours, wherein the weight ratio of the crystal H-type phosphorus pentoxide and ammonia supplying compound is 1:0.01-0.05;

  3. Claim 3Independent Claim

    transferring the malaxator contents resulting from s

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗