Nanoparticle composition and methods of making the same

18Forward Citations (#5049317 Global)
1.4/yrCitation Velocity (#4084024 Global)
2.05Citation PageRank (#14001976 Global)
25Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of fabricating copper nanoparticles includes heating a copper salt solution that includes a copper salt, an N,N-dialkylethylenediamine, and a C6-C18 alkylamine in an organic solvent to a temperature between about 30° C. to about 50° C.; heating a reducing agent solution that includes a reducing agent, an N,N-dialkylethylenediamine, and a C6-C18 alkylamine in an organic solvent to a temperature between about 30° C. to about 50° C.; and adding the heated copper salt solution to the heated reducing agent solution, thereby producing copper nanoparticles. A composition includes copper nanoparticles, a C6-C18 alkylamine and an N,N′-dialkylethylenediamine ligand. Such copper nanoparticles in this composition have a fusion temperature between about 100° C. to about 200° C. A surfactant system for the stabilizing copper nanoparticles includes an N,N′-dialkylethylenediamine and a C6-C18 alkylamine.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 18.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of fabricating copper nanoparticles comprising: heating a copper salt solution comprising a copper salt, an N,N′-dialkylethylenediamine, and a C6-C18 alkylamine in an organic solvent to a temperature between about 30° C. to about 50° C.; heating a reducing agent solution comprising a reducing agent, an N,N′-dialkylethylenediamine, and a C6-C18 alkylamine in an organic solvent to a temperature between about 30° C. to about 50° C.; and adding the heated copper salt solution to the heated reducing agent solution, thereby producing copper nanoparticles.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the copper salt is selected from a copper halide, copper nitrate, copper acetate, copper sulfate, copper formate, and copper oxide.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein the copper halide is selected from copper chlor

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 18 total)

Non-Patent Literature (5)

  • Aslam, et al., "Formation of Cu and Cu2O Nanoparticles by Variation of the Surface Ligand: Preparation, Structure, and Insulating-to-Metallic Transition", Journal of Colloid and Interface Science, 2002, pp. 79-90.
  • Chu et al., "Thermal Aqueous Solution Approach for the Synthesis of Triangular and Hexagonal Gold Nanoplates with Three Different Size Ranges", Inorganic Chemistry, 2006, pp. 808-813, vol. 45.
  • Gupta, Vaibhav, "Synthesis of Metallic Nanoparticles and Their Applications", Department of Research and Advanced Studies of the University of Cincinnati, 2006.
  • Kanninen, et al., "Influence of Ligand Structure on the Stability and Oxidation of Copper Nanoparticles", Journal of Colloid and Interface Science 318 (2008) pp. 88-95.
  • Lisiecki, et al., "Control of the Shape and the Size of Copper Metallic Particles", J. Phys. Chem 1996, 100, pp. 4160-4166.