Cold spray and anodization repair process for restoring worn aluminum parts
Abstract
A method for repairing an aluminum part having a worn portion is provided. In one embodiment, the method includes the steps of: (i) producing a first substantially non-porous coating over the worn portion utilizing a cold spray process wherein a powder mixture is propelled against the worn portion of the aluminum part, and (ii) anodizing the aluminum part to grow an aluminum oxide layer overlaying the first substantially non-porous coating. The powder mixture includes aluminum and an alloy media.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 10.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for repairing an aluminum part having a worn portion, the method comprising: producing a first substantially non-porous coating over the worn portion utilizing a cold spray process wherein a powder mixture is propelled against the worn portion of the aluminum part, the powder mixture containing at least one of pure aluminum and an aluminum alloy and further containing about 5% to about 40% aluminum oxide, by weight of the powder mixture, such that the first substantially non-porous coating produced pursuant to the cold spray process has aluminum oxide particles embedded therein; depos
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗