Method for warm swaging Al-Mg alloy parts
Abstract
A method for the production of swaged aluminum alloy parts, by production of a 0.5 mm-5 mm thick alloy strip made of 1-6 wt. % Mg, <1.2 wt. % Mn, <1 wt. % Cu, <1 wt. % Zn, <3 wt. % Si, <2 wt. % Fe, <0.4 wt. % Cr, Zr<0.3, other elements <0.1 each, total of <0.5, the remainder being Al, cutting a blank from the strip, locally or totally heating the blank at a temperature of 150-350° C. for <30 secs, and swaging the heated blank with the aid of heated tools, at least partially, at a temperature of 150-350° C. in the presence of a lubricant which is compatible with later operations. The swaged parts are automotive body work parts.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 4.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
Process for manufacturing drawn parts made of an aluminum alloy, comprising the steps of: manufacturing of a strip with a thickness of between 0.5 and 5 mm of an alloy with composition consisting essentially of, in % by weight, Mg=1-6, Mn<1.2, Cu<1, Zn<1, Si<3, Fe<2, Cr<0.4, Zr<0.3, other elements <0.1 each and <0.5 total, the remainder being Al; cutting a blank from the strip; heating the blank, locally or completely, for a duration of <30 s, to a temperature of between 150 and 350° C.; and drawing the heated blank using a tool heated at least partially to a temp
- Claim 2Depends on #1
Process according to claim 1 , wherein the strip has an initial strain hardened temper or is partially annealed.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (1)
- Semiatin, S.L., ASM Handbook-Metals Handbook, 1998, ASM International, 9th Edition vol. 14, 576, 579, 827.