High-temperature selective dry etch having reduced post-etch solid residue
Abstract
Methods of dry etching silicon-containing dielectric films are described. The methods include maintaining a relatively high temperature of the dielectric films while etching in order to achieve reduced solid residue on the etched surface. Partially or completely avoiding the accumulation of solid residue increases the etch rate.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of etching a silicon-containing layer on a substrate in a substrate processing region of a substrate processing chamber, the method comprising: flowing a fluorine-containing precursor and a hydrogen-containing precursor into a remote plasma region fluidly coupled to the substrate processing region while forming a plasma in the plasma region to produce plasma effluents; and etching the silicon-containing layer by flowing the plasma effluents into the substrate processing region while maintaining the substrate at a processing temperature between about 60° C. and about 95° C.; and pausin
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (10)
Non-Patent Literature (5)
- "Applied Siconi(TM) Preclean," Applied Materials, Inc., pp. 1-8, printed on Aug. 7, 2009.
- "Applied Siconi™ Preclean," Applied Materials, Inc., pp. 1-8, printed on Aug. 7, 2009.
- "Silicon-Selective Dry Etch for Carbon-Containing Films," U.S. Appl. No. 12/551,180, filed Aug. 31, 2009.
- "Smooth Siconi Etch for Silicon-Containing Films," U.S. Appl. No. 12/646,030, filed Dec. 23, 2009.
- D. Shamiryan et al. Chemical Engineering Communication, vol. 196, (2009), pp. 1475-1535.