Patents
US 8,475,643 B2#66579144 Most CitedExpiredUnited States (USPTO)Utility

Anodic oxidation method and production for titanium oxide coating and method of supporting catalyst

0Forward Citations (#66579144 Global)
0.0/yrCitation Velocity (#66579144 Global)
0.56Citation PageRank (#66579144 Global)
32Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

To provide an anodic oxidation method, a titanium oxide film manufacturing method and a catalyst carrying method which is suitable, for example, for anodic oxidation of aluminum, titanium and catalyst carrying on the surface of alumite (registered trademark), capable of generating an oxide film at a low cost and rapidly by eliminating the use of a strongly acid or strongly basic electrolytic solution and using a carbonated water as an electrolytic solution, capable of controlling the sealing treatment of oxide film through a simple method, capable of effecting the oxide film dyeing and catalyst carrying rationally and easily, and capable of effecting the catalyst carrying safely and surely without eroding a base material. An object ( 3 ) to be treated is electrolyzed in an electrolytic solution received in a treatment vessel ( 1 ) serving the object ( 3 ) as an anodic electrode. It is an anodic oxidation method in which an oxide film is generated on the surface of the object ( 3 ). A carbonated water of a predetermined acid concentration generated by dissolving a pressurized carbon dioxide in a predetermined quantity of water ( 7 ) is used as the electrolytic solution.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An anodic oxidation method comprising the following steps: dissolving supercritical carbon dioxide in water in a sufficient amount to provide a carbonated water having a pH of 3 to 4 as an electrolytic solution; subjecting an object to be treated to anodic electrolysis in the electrolytic solution, in which the object to be treated is the anode, and whereby an oxide film is formed on a surface of the object simultaneous with administering a sealing treatment; immersing the object to be treated in the electrolytic solution for an effective period of time after the oxide film has formed and the

  2. Claim 2Depends on #1

    The anodic oxidation method of claim 1 further comprising the step of depositing a dye or catalyst species in the pores of the oxide fi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (32)

PatentTitleYearCitations
GB 706,739 AMethod of producing hard, abrasion-resistant coatings on aluminum and aluminum alloys—6
US 3,955,556 ACatalytic fluid heater197621
US 4,239,607 AElectrochemical chlorine production process198022
JP S62297497 AMethod for electrolytically coloring aluminum or aluminum alloy—3
JP S6369999 AStirrer for treating liquid—10
JP S6483513 AUltrafine gold particle immobilized alkaline earth metallic compound, production thereof, oxidation catalyst, reduction catalyst and combustible gas sensor element—5
JP H078797 AOxidation catalyst, reduction catalyst and catalyst for combustible gas sensor element and electrode which consist of titanium-based metallic oxide containing superfine particle of gold immobilized thereon—26
US 5,409,156 ASpot-weldable aluminum sheet and production thereof199512
JP H0841686 AFormation of verdigris coating film—8
JP H08246192 AOxidation-treated titanium or titanium-based alloy material having photocatalytic activity and its production—38
US 5,608,267 AMolded plastic semiconductor package including heat spreader1997160
JP H09176892 AAnodization method and device therefor—7
JP H1073227 AManufacture of continuous catalyst body—1
JP H1073226 AManufacture of continuous catalyst body—4
JP H1080622 AGas cleaner—3
US 5,747,180 AElectrochemical synthesis of quasi-periodic quantum dot and nanostructure arrays1998284
JP 2000055794 AAnalyzer for element in sample—13
JP 2000212797 AHighly corrosion-resistant aluminum die-casting material and its anodization method—13
WO 0,077,135 A2Liquid carbon dioxide cleaning utilizing natural and modified natural solvents—15
JP 2001224962 AMethod for manufacturing catalyst by using supercritical fluid and catalyst obtained thereby—11
JP 2001239161 ACatalyst for cleaning up noxious gas at low temperature—19
JP 2001303296 AMetallic material having photocatalytic function and producing method thereof—12
JP 2003071286 ACatalyst for cleaning harmful gas at low temperature—6
JP 2003073868 AMethod for activating surface of base material and apparatus therefor—2
JP 2003183888 AAnodic oxidation method and treatment apparatus therefor—6
WO 03,054,253 A1Anodization method and treating device therefor—3
JP 2003321791 AElectrochemical reaction method—12
EP 1,457,588 A1Anodization method and treating device therefor—7
US 6,869,671 B1Enabling nanostructured materials via multilayer thin film precursor and applications to biosensors200541

Non-Patent Literature (2)

  • F. A. Lowenheim, Electroplating, McGraw-Hill Book Co., 1978, pp. 138-139, 296-299.
  • F. A. Lowenheim, Electroplating, McGraw-Hill Book Company, New York, 1978, pp. 4452-4466.