The present invention relates to a method for forming metal-silicide catalyst nanoparticles with controllable diameter. The method according to embodiments of the invention leads to the formation of ‘active’ metal-suicide catalyst nanoparticles, with which is meant that they are suitable to be used as a catalyst in carbon nanotube growth. The nano-particles are formed on the surface of a substrate or in case the substrate is a porous substrate within the surface of the inner pores of a substrate. The metal-silicide nanoparticles can be Co-silicide, Ni-silicide or Fe-silicide particles. The present invention relates also to a method to form carbon nanotubes (CNT) on metal-silicide nanoparticles, the metal-silicide containing particles hereby acting as catalyst during the growth process, e.g. during the chemical vapor deposition (CVD) process. Starting from very defined metal-containing nanoparticles as catalysts, the diameter of grown CNT can be well controlled and a homogeneous set of CNT will be obtained.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 0.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for forming metal-silicide nanoparticles for use as catalysts in carbon nanotube growth, the method comprising: depositing a barrier layer on a substrate; depositing a thin layer of silicon containing material having a thickness of from 1 nm to 10 nm on the barrier layer; depositing a thin metal film onto the thin layer of silicon containing material, the thin metal film having a thickness of from 1 nm to 10 nm; and annealing the thin metal film and the thin layer of silicon containing material to form metal-silicide nanoparticles having a diameter smaller than 10 nm, wherein the barr

  2. Claim 2Depends on #1

    The method of claim 1 , wherein annealing is performed at a temperature higher than 500° C. and lower than 900° C.

  3. Claim 3Independent Claim

    T

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (1)

Non-Patent Literature (3)

  • Chhowalla et al., J. Appl. Phys. 90 (2001) 5308.
  • De Los Arcos et al., Appl. Phys. Lett. 80(13) (2002) 2383.
  • Teo et al., Appl. Phys. Lett. 79 (2001) 1534.