Patents
US 8,470,194 B2#41651523 Most CitedActiveUnited States (USPTO)Utility

Ni—Zn—Cu ferrite particles, green sheet comprising the Ni—Zn—Cu ferrite particles and Ni—Zn—Cu ferrite sintered ceramics

2Forward Citations (#41651523 Global)
0.1/yrCitation Velocity (#38918781 Global)
0.97Citation PageRank (#43234261 Global)
7Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A Ni—Zn—Cu ferrite material having excellent DC bias characteristics is provided by adding zinc silicate thereto. The above problem can be solved by Ni—Zn—Cu ferrite particles which comprise a spinel-type ferrite and zinc silicate, which have a composition comprising 36.0 to 48.5 mol % of Fe 2 O 3 , 7.0 to 38 mol % of NiO, 4.5 to 40 mol % of ZnO, 5.0 to 17 mol % of CuO and 1.0 to 8.0 mol % of SiO 2 , all amounts being calculated in terms of the respective oxides, and which have a ratio of an X-ray diffraction intensity from a 113 plane of the zinc silicate to an X-ray diffraction intensity from a 311 plane of the spinel-type ferrite is 0.01 to 0.12; a green sheet obtained by forming a material comprising the Ni—Zn—Cu ferrite particles into a film; and a Ni—Zn—Cu ferrite sintered ceramics.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 2.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Particle mixtures comprising zinc silicate particles and Ni—Zn—Cu ferrite particles which comprise a spinel-type ferrite and zinc silicate, which have a composition comprising 36.0 to 48.5 mol % of Fe 2 O 3 , 7.0 to 37 mol % of NiO, 4.5 to 40 mol % of ZnO, 5.0 to 17 mol % of CuO and 1.0 to 8.0 mol % of SiO 2 , all amounts being calculated in terms of the respective oxides, and which have a ratio of an X-ray diffraction intensity from a 113 plane of the zinc silicate to an X-ray diffraction intensity from a 311 plane of the spinel-type ferrite is 0.01 to 0.12.

  2. Claim 2Depends on #1

    A mixture of particles as defined in claim 1 , and a binder material.

  3. Claim 3Independent Claim

    A Ni—Zn—Cu ferrite sintered ceramic which comprises a spinel-type ferrite and zinc silicate, which has a composition comprising 36.0 to 48.5 mol % of Fe 2 O 3 , 7.0 to 38 mol

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Extended European Search Report in EP 08 75 1590 dated Mar. 22, 2012.
  • International Search Report for PCT/JP2008/001046, mailed May 27, 2008.
  • Kumagai et al, "Stress-Insensitive Ferrite for Microinductors", Crystal Properties and Preparation 1989 Fifth International Conference on Ferrites, Jan. 10-13, 1989, Bombay, vol. 27-30, Jan. 1, 1989, pp. 625-630, XP008149705.
  • Official Action and English translation in JP2008-113137 mailed Aug. 8, 2012.
  • Official Action and English translation in JP2008-113137 mailed May 16, 2012.