Patents
US 8,465,872 B2#60807303 Most CitedActiveUnited States (USPTO)Utility

Positive electrode active material sintered body for battery

1Forward Citations (#60807303 Global)
0.1/yrCitation Velocity (#49595376 Global)
0.76Citation PageRank (#60807303 Global)
21Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The positive electrode active material sintered body for a battery of the present invention is a positive electrode active material sintered body for a battery satisfying the following requirements (I) to (VII): (I) fine particles in a positive electrode active material are sintered to constitute the sintered body; (II) a peak pore diameter which provides a maximum differential pore volume value in a pore diameter range of 0.01 to 10 μm in a pore distribution is 0.3 to 5 μm; (III) a total pore volume is 0.1 to 1 cc/g; (IV) an average particle diameter is not less than the peak pore diameter and not more than 20 μm; (V) any peak, which provides a differential pore volume value of not less than 10% of the maximum differential pore volume value, is not present on a smaller pore diameter side than the peak pore diameter in the pore distribution; (VI) a BET specific surface area is 1 to 6 m 2 /g; and (VII) a full width at half maximum of a strongest X-ray diffraction peak is 0.13 to 0.2.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A positive electrode active material sintered body for a battery satisfying the following requirements (I) to (VII): (I) fine particles in a positive electrode active material and carbon particles are sintered to constitute the sintered body; (II) a peak pore diameter which provides a maximum differential pore volume value in a pore diameter range of 0.01 to 10 μm in a pore distribution measured by a mercury porosimeter is 0.3 to 5 μm; (III) a total pore volume measured by the mercury porosimeter is 0.1 to 1 cc/g; (IV) an average particle diameter in laser diffraction/scattering particle diame

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
JP H08180904 ANonaqueous electrolyte secondary battery—21
US 5,709,969 ANon-aqueous electrolyte secondary cell199817
WO 9,828,804 A1Nonaqueous electrolyte secondary battery—57
JP 2000164217 ALithium battery—22
JP 2001143687 APositive electrode for non-aqueous secondary cell—24
US 2001019798 A1Non-aqueous electrolyte secondary battery—26
US 6,287,728 B1Nonaqueous electrolyte secondary battery200160
US 2001025946 A1Lithium manganese oxide spinel compound and method of preparing same—6
JP 2002104827 ASpinel type lithium manganese compound oxide and its manufacturing method and lithium ion secondary battery esing it—16
EP 1,204,601 B1Lithium oxide containing lithium intercalation compounds20033
JP 2003132882 AElectrode material for lithium battery and lithium battery using the same—17
US 2003129496 A1Cathode active material for a lithium secondary battery and a manufacturing method therefor and a lithium secondary battery using said active material and a setup module of said lithium secondary battery using said cathode active material—49
JP 2004083388 ALithium manganese composite oxide granule secondary particle and method for producing the same and application thereof—57
JP 2005050684 AMANUFACTURING METHOD OF CARBON COMPLEX OF LITHIUM-IRON-PHOSPHOR GROUP COMPLEX OXIDE CONTAINING Mn ATOM—37
JP 2005158401 APositive electrode active material, its manufacturing method, and lithium-ion secondary battery—40
JP 2006164859 APositive electrode material for lithium secondary battery, its manufacturing method and lithium secondary battery—35
US 2006141361 A1Positive electrode material for lithium secondary battery, production method thereof, and lithium secondary battery—38
US 7,217,406 B2Lithium-manganese composite oxide granular secondary particle, method for production thereof and use thereof200711
JP 2008063213 AMethod of manufacturing lithium manganate—18
EP 2,110,872 A1Lithium transition metal compound powder, process for production thereof, spray-dried product useful as firing precursor, and positive electrode for lithium secondary battery and lithium secondary battery made by using the same—18
EP 2,144,313 A1Process for producing active material for positive electrode for battery—4

Non-Patent Literature (5)

  • Chinese Office Action, dated Jun. 16, 2011, for Chinese Application No. 200880010270.3.
  • English translation of International Preliminary Report on Patentability (Form PCT/IB/338 and 373) and Written Opinion of the International Searching Authority (Form PCT/ISA/237) mailed on Oct. 22, 2009 in PCT/JP2008/056876.
  • Extended European Search Report for Application No. 08739979.6 dated Jun. 22, 2012.
  • Japanese Office Action dated Dec. 6, 2012 issued in connection with corresponding Japanese Application No. 2008-099414.
  • Machine translation of JP 2008063213.