Patents
US 8,449,795 B2#26174850 Most CitedActiveUnited States (USPTO)Utility

Method of manufacturing sinter-active U3O8 powder and method of producing nuclear fuel pellets utilizing the same

4Forward Citations (#26174850 Global)
0.3/yrCitation Velocity (#25321908 Global)
1.23Citation PageRank (#30913465 Global)
17Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

There is provided a method of producing U 3 O 8 powder having large surface area and small particle size by oxidizing defective UO 2 pellets and manufacturing nuclear fuel pellets which are stable in a pore structure and high in density through the use of a mixture comprising UO 2 powder and U 3 O 8 powder. The method includes producing an U308 powder having a surface area of at least 1 m 2 /g by oxidizing defective UO 2 pellets at a temperature of 300 to 370° C. in such a way that a maximum weight increase rate per 1 g of the UO 2 pellets is up to 0.06 wt %/min; producing a mixed powder by mixing the U 3 O 8 powder with an UO 2 powder by 2 to 15 wt %; producing a compact by compression molding the mixed powder; and sintering the compact in a reducing gas atmosphere at a temperature of 1600 to 1800° C. In addition, a small amount of an Al-compound may be added to the oxidized U 3 O 8 powder before the U 3 O 8 powder is mixed with the UO 2 powder. The additive such as Al is mixed with the U 3 O 8 powder and then mixed with the UO 2 powder to produce the pellets by a conventional production method. This ensures a stable pore structure, high density and a considerable increase in a cr

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing nuclear fuel pellets, the method comprising: producing an U 3 O 8 powder having a surface area of more than 1 m 2 /g and having dominantly a plate shape by oxidizing UO 2 pellets at a temperature of 300 to 370° C. in such a way that a maximum weight increase rate per 1 g of the UO 2 pellets is up to 0.06 wt %/min; producing a mixed powder by mixing the U 3 O 8 powder with an UO 2 powder so that a quaintly of the U 3 O 8 powder is 2 to 15% by weight of the UO 2 powder; producing a compact by compression molding the mixed powder; and sintering the compact in a reducin

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the reducing gas c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Office Action dated Dec. 14, 2010, issued in Japanese Patent Application No. 2007-311935.
  • R.J. McEachern, et al, "A Review of the Oxidation of Uranium Dioxide at Temperatures Below 400°C," Journal of Nuclear Materials, 1998, pp. 87-121, 254.