Embodiments of the invention generally relate to methods for treating a silicon-containing material on a substrate surface and performing a chamber clean process. In one embodiment, a method includes positioning a substrate containing a silicon material having a contaminant thereon within a process chamber and exposing the substrate to an etching gas containing chlorine gas and a silicon source gas while removing the contaminant and maintaining a temperature of the substrate within a range from about 500° C. to less than about 800° C. during an etching process. The method further includes exposing the substrate to a deposition gas after the etching process during a deposition process and exposing the process chamber to a chamber clean gas containing chlorine gas and the silicon source gas after the deposition process during a chamber clean process. The chamber clean process limits the etching of quartz and metal surfaces within the process chamber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for treating a silicon-containing material on a substrate surface, comprising: positioning a substrate comprising a silicon material containing a contaminant within a process chamber; exposing the substrate to an etching gas comprising chlorine gas and a silicon source gas while removing the contaminant and maintaining a temperature of the substrate within a range from about 500° C. to less than about 800° C. during an etching process; exposing the substrate to a deposition gas after the etching process during a deposition process; and exposing the process chamber to a chamber clean g

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the temperature of the substrate is within a range from about 600° C. to less

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,663,831 AMethod of forming transistors with poly-sidewall contacts utilizing deposition of polycrystalline and insulating layers combined with selective etching and oxidation of said layers1987151
US 4,834,831 AMethod for growing single crystal thin films of element semiconductor1989255
US 5,028,560 AMethod for forming a thin layer on a semiconductor substrate199169
US 5,112,439 AMethod for selectively depositing material on substrates1992134
US 5,129,958 ACleaning method for semiconductor wafer processing apparatus1992125
US 5,273,930 AMethod of forming a non-selective silicon-germanium epitaxial film1993126
US 5,288,658 AProcess for the formation of an amorphous silicon deposited film with intermittent irradiation of inert gas plasma199460
US 5,294,286 AProcess for forming a thin film of silicon1994295
US 5,308,788 ATemperature controlled process for the epitaxial growth of a film of material199453
US 5,372,860 ASilicon device production199463
US 5,374,570 AMethod of manufacturing active matrix display device using insulation layer formed by the ale method1994213
US 5,469,806 AMethod for epitaxial growth of semiconductor crystal by using halogenide199554
US 5,480,818 AMethod for forming a film and method for manufacturing a thin film transistor1996348
US 5,503,875 AFilm forming method wherein a partial pressure of a reaction byproduct in a processing container is reduced temporarily1996216
US 5,521,126 AMethod of fabricating semiconductor devices1996141
US 5,527,733 AImpurity doping method with adsorbed diffusion source199684
US 5,674,304 AMethod of heat-treating a glass substrate1997192
US 5,693,139 AGrowth of doped semiconductor monolayers1997163
US 5,796,116 AThin-film semiconductor device including a semiconductor film with high field-effect mobility1998194
US 5,807,792 AUniform distribution of reactants in a device layer1998149
US 5,906,680 AMethod and apparatus for low temperature, low pressure chemical vapor deposition of epitaxial silicon layers1999105
US 5,908,307 AFabrication method for reduced-dimension FET devices1999111
US 5,916,365 ASequential chemical vapor deposition1999819
US 5,983,906 AMethods and apparatus for a cleaning process in a high temperature, corrosive, plasma environment1999128
US 6,025,627 AAlternate method and structure for improved floating gate tunneling devices2000267
US 6,042,654 AMethod of cleaning CVD cold-wall chamber and exhaust lines2000116
US 6,124,158 AMethod of reducing carbon contamination of a thin dielectric film by using gaseous organic precursors, inert gas, and ozone to react with carbon contaminants2000197