Abstract

The invention relates to a lithium vanadium oxide which corresponds to the formula Li 1+α V 3 O 8 (0.1≦α≦0.25). It is composed of agglomerates of small needles having a length l from 400 to 1000 nm, a width w such that 10<l/w<100 and a thickness t such that 10<l/t<100. It is obtained by a process consisting in preparing a precursor gel by bringing α-V 2 O 5 and a Li precursor into contact in amounts such that the ratio of the concentrations [V 2 O 5 ]/[Li] is between 1.15 and 1.5 and in subjecting the gel to a heat treatment comprising a first stage at 80° C.-150° C. for 3 h to 15 days and a second stage between 250° C. and 350° C. for 4 min to 1 hour, under a nitrogen or argon atmosphere. It is useful as an active material of a positive electrode.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of an oxide Li 1+α V 3 O 8 (0≦α≦0.25) comprising preparing a precursor gel and subjecting said gel to a heat treatment, wherein: the precursor gel is prepared by bringing α-V 2 O 5 and a Li precursor into contact in a reaction medium in amounts such that the ratio of the [V 2 O 5 ]/[Li] concentrations is between 1.15 and 1.5; and the heat treatment is carried out in two stages: a first stage under air at a temperature of between 80° C. and 150° C. for a time of 3 hours to 15 days and a second stage under a nitrogen or argon atmosphere at a temperature of between

  2. Claim 2Depends on #1

    The process as claimed in claim 1 , wherein the Li precursor is LiOH.H 2 O and α-V 2 O 5 and LiOH.H 2 O are introduced in water under a nitrogen atmosphere.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (3)

  • International Search Report dated Mar. 8, 2006.
  • Jinggang Xie et al., "Low-Temperature Sol-Gel Synthesis of Li1.2V3O8 from V2O5 Gel", Materials Letters, vol. 57, No. 18, 2003, pp. 2682-2687.
  • Severine Jouanneau et al., "Influence of the Morphology on the Li Insertion Properties of Li1.1V3O8", Journal of Materials Chemistry, vol. 13, 2003, pp. 921-927.