US 8,435,474 B2#14037858 Most CitedActiveUnited States (USPTO)Utility

Surface-treated metal oxide particles

8Forward Citations (#14037858 Global)
0.6/yrCitation Velocity (#12876354 Global)
1.28Citation PageRank (#29271193 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention provides metal oxide particles surface-treated with at least one alkoxysilane compound, methods of making such, and toners comprising same.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A particle composition comprising metal oxide particles surface-treated with at least one alkoxysilane compound, which surface-treated metal oxide particles are hydrophobic, non-aggregated, and have a tap density of about 110 g/l to about 420 g/l, and a BET surface area of about 200 m 2 /g or less, and wherein a solid-state Si nuclear magnetic resonance spectrum of the surface-treated metal oxide particles exhibits a ratio T3:T2 of about 2 or more, wherein T2 is the integrated intensity of a peak having a chemical shift in the CP/MAS 29 Si NMR spectrum centered within the range of −56 ppm to −

  2. Claim 2Depends on #1

    The composition of claim 1 , wherein the at least one alkoxysil

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,900,588 ANon-filming dual additive developer197561
US 4,845,004 AFluidity improver for positively-charging resin powder198928
US 4,923,520 ASpherical fused silica and its use in fillers and resin compositions199071
US 4,943,507 AToner for developing electrostatic latent image and method for developing electrostatic latent image with the same199016
US 4,950,502 AMethod of hydrophobing silica199037
US 4,985,477 AMethod of producing treated silica filler for silicone rubber199167
US 5,008,305 ATreated silica for reinforcing silicone elastomer199159
US 5,009,874 AHydrophobic precipitated silica granules199176
US 5,013,585 AMethod for the preparation of surface-modified silica particles199186
US 5,024,915 APositively chargeable developer199130
US 5,039,736 AMethod for the preparation of an organopolysiloxane composition199117
US 5,096,733 APrevention of the acute cytotoxicity associated with silica containing minerals199223
US 5,135,832 AColored toner compositions199237
US 5,194,356 AToner compositions199344
EP 0,371,147 B1Abrasive composition for silicon wafer19936
US 5,226,930 AMethod for preventing agglomeration of colloidal silica and silicon wafer polishing composition using the same199348
US 5,266,432 AHydrophobic polyester toner composition199325
US 5,320,925 AElectrophotographic toner composition199411
US 5,376,172 AMetal oxide processes and toners thereof199447
US 5,415,936 ASurface-modified pyrogenically produced titanium dioxide199532
US 5,422,214 ADry toner for developing electrostatic latent image, process for producing same, and image formation process using same199544
US 5,424,161 AToner composition199519