Patents
US 8,429,960 B2#33616503 Most CitedActiveUnited States (USPTO)Utility

Process for measuring an adhesion energy, and associated substrates

3Forward Citations (#33616503 Global)
0.2/yrCitation Velocity (#31051978 Global)
1.02Citation PageRank (#40451004 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a structure and a process for measuring an energy of adhesion between two substrates bonded in a transverse direction. The method involves providing for at least one of the two substrates to have a plurality of elementary test cells within a test layer each being capable of locally applying, in the transverse direction, a preset mechanical stress (σ), dependent on the temperature (T), to a bond interface between the substrates in a direction tending to separate them, applying a test temperature to the substrates and identifying debonded regions of the bond interface so that the local adhesion energy at the test temperature in the regions may be deduced therefrom, the local adhesion energy in a region of the bond interface being deduced from the stress applied by the test cells that caused debonding in the region.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for measuring an energy of adhesion between two bonded substrates which comprises: providing a test layer on a first substrate, wherein the test layer has an exposed surface; providing a plurality of elementary test cells within the test layer for locally applying a preset mechanical stress (σ) dependent on a temperature (T); bonding a second substrate to the exposed surface of the test layer to form a bonding interface; and increasing the temperature (T) of the bonded substrates to up to a test temperature (T t ), wherein the plurality of elementary test cells apply a preset transve

  2. Claim 2Depends on #1

    The process of claim 1 , which further comprises providing a bonding layer on the exposed surface of the test layer, and bonding the second substrate t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
EP 0,366,208 A2Method for bonding silicon wafers together, for manufacturing semiconductor devices—10
JP H0389519 AManufacture of semiconductor substrate—9
EP 0,451,993 A2Method for preparing a substrate for semiconductor devices—32
JP H04263425 AGrinding device for semiconductor substrate and method thereof—38
US 5,223,001 AVacuum processing apparatus1993120
JP H0745485 AFabrication of bonded semiconductor substrate—17
US 5,537,884 AMethod for measuring adhesion strength of resin material199618
JP H0917984 ABonded soi substrate manufacturing method—22
EP 0,444,942 B1A bonded wafer and a method of manufacturing it19975
US 5,696,327 AMethod and apparatus for separating a thin film from a substrate199732
US 5,834,812 AEdge stripped BESOI wafer199841
JP H1117701 ACommunication time shortening system for satellite intranet service—13
JP H1167701 AManufacture of bonded soi board and protective agent applying apparatus—20
US 5,937,312 ASingle-etch stop process for the manufacture of silicon-on-insulator wafers1999101
WO 9,960,607 A2Tool for wafer bonding in a vacuum—12
EP 0,964,436 A2Method for manufacturing SOI wafer and SOI wafer—27
JP H11354761 ASoi substrate and its production—15
US 6,008,113 AProcess for wafer bonding in a vacuum199959
US 6,113,721 AMethod of bonding a semiconductor wafer200035
US 6,117,695 AApparatus and method for testing a flip chip integrated circuit package adhesive layer200042
JP 3,089,519 B2衛星通信方式20002
US 6,180,496 B1In situ plasma wafer bonding method2001185
US 6,207,005 B1Cluster tool apparatus using plasma immersion ion implantation2001114
US 6,221,774 B1Method for surface treatment of substrates200142
JP 2001144274 AMethod for producing semiconductor substrate—12
US 2001055863 A1Methods for manufacturing soi wafer and soi wafer—27
US 6,347,284 B1System for prediction of adhesion energy at interface between dissimilar materials and method thereof20027

Non-Patent Literature (5)

  • Andreas Plöbetal et al., "Covalent Silicon Bonding at Room Temperature in Ultra High Vacuum", Mat. Res. Soc. Symp. Proc., vol. 483, pp. 141-146, Materials Research Society (1998).
  • Andreas Plöβl et al., "Covalent Silicon Bonding at Room Temperature in Ultra High Vacuum", Mat. Res. Soc. Symp. Proc., vol. 483, pp. 141-146, Materials Research Society (1998).
  • Burns, James A. et al., "A Wafer-Scale 3-D Circuit Integration Technology", IEEE Transactions on Electron Devices, vol. 53, No. 10, pp. 2507-2516 (2006).
  • European Search Report for EP08291226 dated Jul. 7, 2009.
  • European Search Report, French Appln. No. 1002618, dated Jan. 25, 2011.