Stress locking layer for reliable metallization
Abstract
Recrystallization and grain growth of metal, such as Cu, is achieved at higher anneal temperatures of 150° C. to 400° C., for example, for short anneal times of five to sixty minutes by forming a metal stress locking layer on the Cu before anneal and chemical-mechanical polishing. The stress locking layer extends the elastic region of the Cu by suppressing atom diffusion to the free surface, resulting in near zero tensile stress at room temperature after anneal. Stress voiding, which creates reliability problems, is thereby avoided. Improved grain size and texture are also achieved. The stress locking layer is removed after anneal by chemical-mechanical polishing leaving the Cu interconnect with low stress and improved grain size and texture.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 11.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for forming an electrical interconnect structure, comprising: providing a dielectric substrate with a trench; conformally forming an interconnect layer of Cu on said substrate and in said trench with said layer of Cu having small multiple grain size structure providing multiple grain boundaries that act as fast diffusion paths during electromigration; forming a stress locking layer directly on said layer of Cu on said substrate and in said trench to lock stress and extend an elastic region of said layer of Cu during annealing so that relaxation by surface diffusion is reduced; then an
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗