Method for producing sintered NdFeB magnet
Abstract
The present invention provides a method for producing a sintered NdFeB magnet having high coercivity and capable of being brought into applications without lowering its residual magnetic flux density or maximum energy product and without reprocessing. The method for producing a sintered NdFeB magnet according to the present invention includes applying a substance containing dysprosium (Dy) and/or terbium (Tb) to the surface of the sintered NdFeB magnet forming a base body and then heating the magnet to diffuse Dy and/or Tb through the grain boundary and thereby increase the coercivity of the magnet. This method is characterized in that: (1) the substance containing Dy or Tb to be applied to the surface of the sintered NdFeB magnet is substantially a metal powder; (2) the metal powder is composed of a rare-earth element R and an iron-group transition element T, or composed of R, T and another element X, the element X capable of forming an alloy or intermetallic compound with R and/or T; and (3) the oxygen content of the sintered NdFeB magnet forming the base body is 5000 ppm or lower. The element T may contain nickel (Ni) or cobalt (Co) to produce an anticorrosion effect.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 0.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for producing a sintered NdFeB magnet, comprising: applying a substance to a surface of the sintered NdFeB magnet, the substance being substantially a metal powder comprising (i) a rare earth element component (R) that is dysprosium and/or terbium and optionally at least one other rare earth element and (ii) an iron group transition element component (T) that is at least one member selected from the group consisting of iron, cobalt, and nickel; and then heating the magnet to diffuse dysprosium and/or terbium through grain boundaries of the magnet in order to increase coercivity of the
- Claim 2Depends on #1
The method for producing a sintered NdFeB magnet according to claim 1 , wherein the oxygen content is 4000 ppm or lower.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (17)
Non-Patent Literature (5)
- Extended Search Report issued in corresponding European Patent Application No. 07790283.1 dated Apr. 6, 2011.
- Fukuda et al., "Magnetic Properties and Corrosion Characteristics of Nd-(Fe, Co, Ni)-B Pseudo-Ternary Systems", Kawasaki Steel Technical Report, 1989, pp. 312-315, vol. 21., No. 4.
- Hirota et al., "Increase in Coercivity of Sintered NdFeB Magnet by Grain Boundary Diffusion Method", Abstracts of Autumn Meeting of Japan Society of Powder and Powder Metallurgy, 2005, p. 143.
- Hirota et al., "Increase in Coercivity of Sintered NdFeB Magnet by Grain Boundary Diffusion Method", Speech Summaries of 2005 Spring Meeting of Japan Society of Powder and Powder Metallurgy, 2005, p. 143.
- Ishigaki et al., "Surface Improvements on Magnetic Properties of Small-Sized Nd-Fe-B Sintered Magnets", Neomax Technical Report, 2005, pp. 15-19, vol. 15.