US 8,415,772 B2#22206610 Most CitedActiveUnited States (USPTO)Utility

Method to prevent surface decomposition of III-V compound semiconductors

5Forward Citations (#22206610 Global)
0.4/yrCitation Velocity (#21339793 Global)
1.22Citation PageRank (#31121368 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of preventing surface decomposition of a III-V compound semiconductor is provided. The method includes forming a silicon film having a thickness from 10 Å to 400 Å on a surface of an III-V compound semiconductor. After forming the silicon film onto the surface of the III-V compound semiconductor, a high performance semiconductor device including, for example, a MOSFET, can be formed on the capped/passivated III-V compound semiconductor. During the MOSFET fabrication, a high k dielectric can be formed on the capped/passivated III-V compound semiconductor and thereafter, activated source and drain regions can be formed into the III-V compound semiconductor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A semiconductor structure comprising: a polycrystalline silicon layer having a thickness from 70 Å to 380 Å located directly on a surface of a III-V compound semiconductor, wherein the III-V compound semiconductor has a surface layer at the interface with the polycrystalline silicon layer that has no surface pitting caused by evaporation of a Group V element from the III-V compound semiconductor, a surface roughness of less than 240 nm and a root mean square roughness of less than 0.5 nm.

  2. Claim 2Depends on #1

    The semiconductor structure of claim 1 further comprising a high k dielectric material atop at least a portion of said silicon layer.

  3. Claim 3Depends on #1

    The semiconductor structure of claim 1 wherein said thickness of said silicon layer is from 150 Å to 275 Å.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Molarius, J.M., et al., "Tantalum-based Encapsulants for Thermal Annealing of GaAs" Journal of the Electrochemical Society, Mar. 1997, pp. 834-837, vol. 138.