Non-fibrous polymer solution of para-aramid with high relative viscosity
Abstract
The invention relates to a non-fibrous polymer solution essentially consisting of 1 to 8 wt. % para-aramid, at least 50 mole % of the aromatic moieties thereof being unsubstituted, in a mixture of a) a polar amide solvent selected from N-methyl-2-pyrrolidone, N,N′-dimethylformamide, N,N′-dimethylacetamide, tetramethylurea, and mixtures thereof; b) between 0.7 mole of an alkali or earth alkali chloride per mole amide groups of the para-aramid and 7.5 wt. % of the alkali or earth alkali chloride, and c) water; and wherein at least 50 wt. % of the formed hydrochloric acid has been neutralized to obtain a solution having a dynamic viscosity which is at least a factor three smaller than the dynamic viscosity of the polymer solution without neutralization. The invention further pertains to a process making the same and para-aramid pulp-like fiber, paper and film made from said polymer solution.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A non-fibrous polymer solution, the polymer solution comprising: 1 to 6 wt. % poly(paraphenylene terephthalamide) (PPTA), obtained from polymerizing para-phenylenediamine and terephthaloyl dichloride under a formation of hydrochloric acid, a polar amide solvent selected from the group consisting of N-methyl-2-pyrrolidone (NMP), N,N′-dimethylformamide, N,N′-dimethylacetamide (DMAc), tetramethylurea, and mixtures thereof; an alkali or an alkaline earth metal chloride selected from the group consisting of lithium chloride (LiCl) and calcium chloride (CaCl 2 ), in an amount of from 0.7 mole per mo
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗