Heat stable halogen-free flame retardant copolyester thermoplastic elastomer compositions
Abstract
Halogen-free flame retardant compositions exhibiting flame retardance and retention of mechanical properties, especially elongation at break, upon long-term high temperature exposure and comprising a) at least one copolyester thermoplastic elastomer, and b) from at or about 1 to at or about 30 weight percent, based on the total weight of the composition, of at least one flame retardant comprising a phosphinate, diphosphinate and/or polymers of these; c) from at or about 0.25 to at or about 15 weight percent, based on the total weight of the flame retardant composition, of one or more polyhydroxy polymers having a number average molecular weight of at least 2000 and selected from the group consisting of ethylene vinyl alcohol copolymers and poly(vinyl alcohol)s.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A flame retardant composition comprising: A. at least one copolyester thermoplastic elastomer; B. from at or about 1 to at or about 30 weight percent, based on the total weight of the flame retardant composition, of at least one flame retardant selected from the group consisting of phosphinates of formula I, diphosphinates of formula II, polymers thereof and combinations of two or more thereof wherein R 1 and R 2 are independently selected from the group consisting of hydrogen, linear or branched C 1 -C 6 alkyl groups, and aryl groups; R 3 is a linear or branched C 1 -C 10 -alkylene group,
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (17)
Non-Patent Literature (1)
- Kohout, Strength Changes of Moulded Polymide Composite Caused by Thermal Oxidation, Journal of Materials Science, 1999, 34, 843-849, Kluwer Academic Publishers.