Apparatus and method for controlling silicon nitride etching tank
Abstract
A method and system for controlling a silicon nitride etching bath provides the etching bath including phosphoric acid heated to an elevated temperature. The concentration of silicon in the phosphoric acid is controlled to maintain a desired level associated with a desired silicon nitride/silicon oxide etch selectivity. Silicon concentration is measured while the silicon remains in soluble form and prior to silica precipitation. Responsive to the measuring, fresh heated phosphoric acid is added to the etching bath when necessary to maintain the desired concentration and silicon nitride:silicon oxide etch selectivity and prevent silica precipitation. The addition of fresh heated phosphoric acid enables the etching bath to remain at a steady state temperature. Atomic absorption spectroscopy may be used to monitor the silicon concentration which may be obtained by diluting a sample of phosphoric acid with cold deionized water and measuring before silica precipitation occurs.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 11.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for controlling an etching bath comprising: providing a batch etching bath configured to process a batch of wafers therein, said batch etching bath containing phosphoric acid heated to an elevated bath temperature, said batch etching bath including an inner tank for processing said batch of wafers therein, and an outer tank; measuring silicon concentration of silicon in said phosphoric acid contained in said batch etching bath while said silicon is in soluble form; and responsive to said measuring, controlling said silicon concentration by adding fresh heated phosphoric acid to said p
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗