High-strength pearlitic steel rail having excellent delayed fracture properties
Abstract
The invention provides a high-strength pearlitic steel rail, which is inexpensive, and has a tensile strength of 1200 MPa or more, and is excellent in delayed fracture properties. Specifically, the rail contains, in mass percent, C of 0.6 to 1.0%, Si of 0.1 to 1.5%, Mn of 0.4 to 2.0%, P of 0.035% or less, S of 0.0005 to 0.010%, and the remainder is Fe and inevitable impurities, wherein tensile strength is 1200 MPa or more, and size of a long side of an A type inclusion is 250 mm or less in at least a cross-section in a longitudinal direction of a rail head, and the number of A type inclusions, each having a size of a long side of 1 mm to 250 mm, is less than 25 per observed area of 1 mm 2 in the cross-section in the longitudinal direction of the rail head.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A pearlitic steel rail having a composition consisting of, in mass percent, 0.6 to 1.0% of C, 0.1 to 1.5% of Si, 0.4 to 2.0% of Mn, 0.035% or less of P, 0.0005 to 0.010% of S, optionally 0.004% or less of O, optionally 0.001 to 0.01% of Ca, optionally one or more elements selected from the group consisting of 0.5% or less of V, 1.5% or less of Cr, 1.0% or less of Cu, 1.0% or less of Ni, 0.05% or less of Nb, 1.0% or less of Mo, and 1.0% or less of W, no more than 2 ppm hydrogen, and the remainder being Fe and inevitable impurities, wherein the tensile strength is 1200 MPa or more, and the size
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 9,670,570 B2 | High carbon steel rail with enhanced ductility | 2017 | 1 |
| US 10,196,781 B2 | Hypereutectoid steel rail and preparation method thereof | 2019 | 1 |
References Cited — Backward Prior Art (23)
Non-Patent Literature (1)
- Canadian Office Action dated Sep. 14, 2011 for Canadian Patent Application No. 2,645,858.