Stabilized ceramic composition, apparatus and methods of using the same
Abstract
In one aspect, the invention includes a refractory material, said material comprising: (i) at least 20 wt. % of a first grain mode stabilized zirconia based upon the total weight of said material, said first grain mode having a D50 grain size in the range of from 5 to 2000 μm, said stabilized zirconia including a matrix oxide stabilizer; (ii) at least 1 wt. % of a second grain mode having a D50 grain size in the range of from 0.01 μm up to not greater than one-fourth the D50 grain size of said first grain mode zirconia, based upon the total weight of said material; and (iii) at least 1 wt. % of a preservative component within at least one of said first grain mode stabilized zirconia, said second grain mode stabilized zirconia, and an optional another grain mode; wherein after sintering, said material has porosity at 20° C. in the range of from 5 to 45 vol %.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A refractory material comprising: (i) at least 20 wt. % of a first grain mode based upon the total weight of said refractory material, said first grain mode comprising stabilized zirconia having a D50 grain size in the range of from 5 to 2000 μm, said stabilized zirconia including a matrix oxide stabilizer; (ii) at least 1 wt. % of a second grain mode having a D50 grain size in the range of from 0.01 μm up to not greater than one-fourth the D50 grain size of said first grain mode zirconia, based upon the total weight of said refractory material, wherein said second grain mode comprises a fully
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Bartholome, V.E., "Methods of Energy Addition for Endothermic Gas Reactions at High Temperatures", Zeitschrift fuer Elektrochemie und Angewandte Physikalische Chemie, 57, pp. 497-502 (1953).
- Bartholome, V.E., "Methods of Energy Addition for Endothermic Gas Reactions at High Temperatures", Zeitschrift fuer Elektrochemie und Angewandte Physikalische Chemie, 57, pp. 497-502 (1953). (With Machine Translation).
- Basu, B. et al., "Microstructure-toughness-wear relationship of tetragonal zirconia ceramics", Journal of the European Ceramic Society, Elsevier Ltd., vol. 24, pp. 2031-2040 (2004).
- Bixler, G.H. et al. "Wulff Process Acetylene", Journal of Industrial and Engineering Chemistry, Washington, D.C., 45, pp. 2596-2606 (1953).
- Bogart, M.J.P. et al., "Recent Developments in Wulff Acetylene", Chemical Engineering Progress, 50, pp. 372-375 (1954).