Lighter than air balloon made from a biaxially oriented polyester film
Abstract
A long life balloon formed from a lamination. The lamination includes a polyester film with a total thickness of 4 μm to 12 μm. The polyester film includes a biaxially oriented polyester core layer and at least one amorphous copolyester skin layer. The lamination also includes a sealant layer and a gas barrier layer on an opposite side of the polyester film from the sealant layer. The oxygen transmission rate of the balloon is less than 0.1 cc/100 sqin/day, a bonding strength of the gas barrier layer to the surface of the polyester film is more than 300 g/in at dry conditions, a sealing strength of the balloon is more than 3.5 kg/in, and a floating time of the balloon is more than 20 days.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 13.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A balloon formed from a lamination, the lamination comprising; a polyester film with a total thickness of 4 μm to 12 μm comprising a biaxially oriented polyester core layer comprising high crystalline polyester and at least one amorphous copolyester skin layer; a sealant layer adjacent to the amorphous copolyester skin layer; and a gas barrier layer on an opposite side of the polyester film from the sealant layer, wherein an oxygen transmission rate of the balloon is less than 0.1 cc/100 sqin/day, a dry bonding strength of the gas barrier layer to the surface of the polyester film is more than
- Claim 2Depends on #1
The balloon of claim 1 , wherein the sealant layer comprises a low density polyethylene.
- Claim 3Depends on #1
The balloon of claim 1 ,
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (13 of 13 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- "Explanation of Results-Biobased Analysis using ASTM D6866," located at (6 pages).
- "Explanation of Results—Biobased Analysis using ASTM D6866," located at <http://www.betalabservices.com/PDF/ASTM-D6866-Example-Report-JP.pdf> (6 pages).
- Bozell et al. (Mar. 2010). "Technology Development for the Production of Biobased Products from Biorefinery Carbohydrates-the US Department of Energy's 'Top 10' Revisited," Green Chemistry 14(4). 539-554.
- Chicarella et al., U.S. Office Action mailed Dec. 23, 2011, directed to U.S. Appl. No. 13/196,554; 6 pages.
- Chicarella et al., U.S. Office Action mailed Jan. 23, 2012, directed to U.S. Appl. No. 13/196,495; 6 pages.