Process of producing flame-retardant silane-crosslinked olefin resin, insulated wire, and process of producing insulated wire

3Forward Citations (#33385729 Global)
0.2/yrCitation Velocity (#31043273 Global)
1.04Citation PageRank (#39468010 Global)
17Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process of producing a flame-retardant silane-crosslinked olefin resin, an insulated wire, and a process of producing an insulated wire. The process includes kneading and molding a silane graft batch containing a silane-grafted olefin resin in which a silane coupling agent is graft polymerized onto an olefin resin, a flame retardant batch in which an olefin resin is mixed with a flame retardant containing metal hydroxide, a catalyst batch in which an olefin resin is mixed with a silane crosslinking catalyst, and water crosslinking the batches after kneading and molding. A mass ratio of the flame retardant batch to the silane graft batch is 60:40 to 90:10, and the catalyst batch amount is 3 to 10 part by mass with respect to 100 part by mass of a component of the silane graft and flame retardant batches. The wire is prepared by covering a conductor with the silane-crosslinked olefin resin.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process of producing a flame-retardant silane-crosslinked olefin resin, the process comprising the steps of: kneading and molding a silane graft batch containing a silane-grafted olefin resin prepared by graft polymerizing a silane coupling agent onto an olefin resin, a flame retardant batch prepared by mixing an olefin resin with a flame retardant containing metal hydroxide, and a catalyst batch prepared by mixing an olefin resin with a silane crosslinking catalyst; and water crosslinking a molding of the batches after the kneading and molding step.

  2. Claim 2Depends on #1

    The process according to claim 1 , wherein: a mass ratio of the flame retardant batch to the silane graft batch is in a range of 60:40 to 90:10; and an amount of the catalyst batch is in a range of 3 to 10 part by mass with respect to 100 part by mass of a component constituted of the silane graft b

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Apr. 26, 2012 Office Action issued in Chinese Application No. 200880018112.2 (with English translation).
  • Chinese Office Action in Chinese Patent Application No. 200880018112.2; dated Dec. 13, 2010 (with English-language translation).
  • International Search Report issued in international application No. PCT/JP2008/060051 on Jun. 24, 2008.
  • Jun. 8, 2011 Office Action issued in German Patent Application No. 11 2008 001 402.7 (with translation).
  • Nov. 15, 2012 Office Action issued in Chinese Patent Application No. 200880018112.2 (with translation).