Semiconductor device fabrication and dry develop process suitable for critical dimension tunability and profile control
Abstract
The critical dimension (CD) of features formed during the fabrication of a semiconductor device may be controlled through the use of a dry develop chemistry comprising O 2 , SO 2 and a hydrogen halide. For example, a dry develop chemistry comprising a gas comprising O 2 and a gas comprising SO 2 and a gas comprising HBr may be used to remove exposed areas of a carbon-based mask. The addition of HBr to the conventional O 2 and SO 2 dry develop chemistry enables a user to tune the critical dimension by growing, trimming and/or sloping the sidewalls and to enhance sidewall passivation and reduce sidewall bowing.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 1.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of fabricating a semiconductor device comprising: forming a mask comprising carbon over a semiconductor device structure; forming a preliminary mask comprising photoresist over at least a portion of the mask; and exposing surfaces of the mask comprising carbon exposed through the preliminary mask comprising photoresist to a dry develop etch chemistry comprising O 2 , SO 2 , and at least one hydrogen halide to remove at least a portion of the mask comprising carbon and form at least one feature in the mask comprising carbon; and adjusting a ratio of the at least one hydrogen halide to
- Claim 2Depends on #1
The method of claim 1 , wherein adjusting a ratio of the at least on
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗