Thermoplastic resin composition and laminate and tire manufactured using the same
Abstract
There is provided a thermoplastic resin composition which comprises a modified rubber having excellent low-temperature durability dispersed in a polyamide resin matrix in order to improve the low-temperature durability or repeated fatigue resistance of the polyamide resin and which maintains its flowability and can be formed into a film even at a high content of the modified rubber, and has excellent low-temperature durability. The thermoplastic resin composition comprises a modified polyamide resin (A) obtained by melt blending 100 parts by weight of a polyamide resin (A1) and 0.05 to 5 parts by weight of a compound (A2) capable of binding to a terminal amino group of the polyamide resin, at a temperature equal to or higher than the melting point of the polyamide resin (A1), and a modified rubber (B) having an acid anhydride group, an epoxy group, or a carboxyl group or a derivative thereof. The compound (A2) is preferably a monofunctional epoxy compound. The film of the thermoplastic resin composition is suitably used for the manufacture of tires and hoses.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 1.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A thermoplastic resin composition comprising a modified polyamide resin matrix (A) obtained by melt blending 100 parts by weight of a polyamide resin (A1) and 0.05 to 5 parts by weight of a monofunctional epoxy compound (A2), at a temperature equal to or higher than the melting point of the polyamide resin (A1), and a rubber (B) having an acid anhydride group, an epoxy group, or a carboxyl group, wherein the rubber (B) is dispersed in the polyamide resin matrix, and further comprising an ethylene-vinyl alcohol copolymer (C).
- Claim 2Depends on #1
The thermoplastic resin composition according to claim 1 , wherein the weight ratio of the modified polyamide resin (A) to the ethylene-vinyl alcohol copolymer (C) is 90/10 to 10/90, and the thermoplastic resin composition comprises 50 to 150 parts by weight of the rubber (B) based on 100 parts by weight of a total of the modified polyamide
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 10,150,336 B2 | Tire with thermoplastic innerliner | 2018 | 1 |
References Cited — Backward Prior Art (18)
Non-Patent Literature (1)
- Extended European Search Report issued in related European Application No. 10193634.2 on Mar. 1, 2012.