Patents
US 8,344,044 B2#24798340 Most CitedActiveUnited States (USPTO)Utility

Glass-containing resin molded product

4Forward Citations (#24798340 Global)
0.3/yrCitation Velocity (#25237214 Global)
1.38Citation PageRank (#26151707 Global)
14Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Provide an agent-to-be-filled/glass-containing resin molded product having no skin layer formed on its surface and free of sink marks, warping and other forms of deformation and also allowing an agent-to-be-filled blended in it to sufficiently effectuate, with a low blending ratio, action equivalent to when the agent-to-be-filled is blended at a traditional blending ratio; wherein the agent-to-be-filled/glass-containing resin molded product is characterized in that it is made of one type of resin selected from the group that includes polyethylene resin, polypropylene resin, polyethylene terephthalate resin and polyamide resin, that it contains solid, spherical glass beads with an average particle size of 10 to 40 μm, and when the glass blending ratio of these solid, spherical glass beads is 40 to 70 percent by weight, no skin layer is formed on the surface of such glass-containing resin molded product as measured by laser Raman spectroscopy, and presence of the aforementioned solid, spherical glass beads and agent-to-be-filled on its surface allows the agent-to-be-filled to effectuate its action.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A glass-containing resin molded product containing an active ingredient, formed by molding, using dies, a glass-containing resin composition produced by meltkneading pellets of thermoplastic resin, solid, spherical glass particles, and the active ingredient, said active ingredient selected from the group consisting of an antibacterial agent, antifungal agent, flame retardant and antistatic agent, wherein the solid, spherical glass particles have an average particle size of 10 to 40 μm and are contained in the glass-containing resin molded product at a glass blending ratio of 40 to 70 percent b

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • Koji Yamada et al., Structural Evaluation of Injection Moldings by Laser-Raman Spectroscopy, Science and Industry vol. 81, No. 9, Sep. 2007, pp. 433-438. (Englishi abstract only).
  • Koyo Arikata, "Anti-Failure Measures in Injection Molding Process", (2) Skin Layer and Fluidized Layer, Nikkan Kogyo Shinbun, Jul. 18, 2006, p. 10, line 1-6, under Fig. 1.9.
  • Sigma Press, "Plastic Materials for Molding Processing", Edited by Polymer Process Society, Feb. 25, 2005, p. 108, line 3-11 under Fig. 32 and p. 109, line 13-16 under Fig. 3.3.