Patents
US 8,330,136 B2#22446428 Most CitedActiveUnited States (USPTO)Utility

High concentration nitrogen-containing germanium telluride based memory devices and processes of making

5Forward Citations (#22446428 Global)
0.4/yrCitation Velocity (#22213318 Global)
1.11Citation PageRank (#36169400 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A PCM device has the composition GexTeyNzAm deposited onto a substrate, where x is about 40% to about 60%, y is about 30% to about 49%, and z is about 5% to about 20% and more preferably about 5% to about 40%. The component represented as A is optional and representative of an element of Sb, Sn, In, Ga, or Zn, and m is up to about 15%. The composition is in the form of a film, and the nitrogen allows for the substantially conformal deposition of the film onto the substrate. A CVD process for depositing the PCM comprises delivering a Ge-based precursor and a Te-based precursor in vapor form to a CVD chamber, heating and pressurizing the chamber, and depositing the film onto a substrate. In making a phase change device using this process, the film is annealed and polished.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A phase change memory device, comprising: a phase change memory material comprising GST and nitrogen, wherein the phase change memory material includes from about 40 to about 60 atomic percent germanium, up to about 15 atomic percent antimony, from about 30 atomic percent to about 49 atomic percent tellurium, and from about 5 to about 15 atomic percent nitrogen, wherein the phase change memory material is conformally deposited on a topographical feature of the substrate.

  2. Claim 2Depends on #1

    The phase change memory device of claim 1 , wherein the phase change memory material includes about 40 atomic percent germanium, and about 49 atomic percent tellurium.

  3. Claim 3Depends on #1

    The phase change memory device of claim 1 , wherein the phase change memory material has resistivity of less than 0.1 ohm-centimeters in the crystalline phase, and resistivity greater than about 10 ohm-

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,467,686 APreparation of organosilicon-nitrogen compounds196937
JP S5838296 ANovel antimony compound—14
US 4,383,119 AOrganomagnesium compounds198331
US 4,491,669 AMixed alkoxyaminosilanes, methods of making same and vulcanizing silicons prepared therefrom198569
US 4,499,198 APolymerization catalysts and methods198531
US 4,895,709 AMethod of preparing metal carbides, nitrides, and the like199040
US 4,927,670 AChemical vapor deposition of mixed metal oxide coatings1990137
US 4,948,623 AMethod of chemical vapor deposition of copper, silver, and gold using a cyclopentadienyl/metal complex199097
US 4,960,916 AOrganometallic antimony compounds useful in chemical vapor deposition processes199079
US 4,962,214 ACatalytic enantioselective addition of hydrocarbon equivalents to alpha, beta-unsaturated carbonyl compounds199043
US 5,003,092 AUse of R2 MR' to prepare semiconductor and ceramic precursors199142
US 5,008,422 APolysilazanes and related compositions, processes and uses199197
US 5,084,588 AReducing halide contamination in alkoxy silanes199228
US 5,139,825 AProcess for chemical vapor deposition of transition metal nitrides1992147
US 5,178,911 AProcess for chemical vapor deposition of main group metal nitrides1993123
US 5,210,254 AAcidic halide neutralization in alkoxysilanes199335
US 5,225,561 ASource reagent compounds for MOCVD of refractory films containing group IIA elements1993180
US 5,268,496 AProcess for the preparation of polysilazanes199324
US 5,312,983 AOrganometallic tellurium compounds useful in chemical vapor deposition processes199431
US 5,417,823 AMetal-nitrides prepared by photolytic/pyrolytic decomposition of metal-amides199521
US 5,442,200 ALow resistance, stable ohmic contacts to silcon carbide, and method of making the same199564
US 5,453,494 AMetal complex source reagents for MOCVD1995265
JP H07263431 AFormation of tantalum-containing high dielectric film—13
US 5,566,045 AHigh-dielectric-constant material electrodes comprising thin platinum layers1996151
US 5,576,928 AHigh-dielectric-constant material electrodes comprising thin platinum layers199678

Non-Patent Literature (4)

  • Abrutis, A., et al., "Hot-Wire Chemical Vapor Deposition of Chalcogenide Materials for Phase Change Memory Applications", "Chem. Mater.", 2008, pp. 3557-3559, vol. 20.
  • Allen, Frank. H. et al., "Tables of Bond Lengths Determined by X-ray and Neutron Diffraction", "J. Chem. Soc. Perkin Tran. II", Feb. 1987, pp. S1-S19.
  • Anderson, Herbert H., "Dialkylaminogermanes and Dialkylaminosilanes", "J. Amer. Chem. Soc.", Mar. 20, 1952, pp. 1421-1423, vol. 74, No. 6.
  • Anderson, Q. et al. , "Synthesis and Characterization of the First Pentaphenylcyclopentadienyl Copper Complex (Ph5CP)Cu(PPh3)", "Organometallics", 1998, pp. 4917-4920, vol. 17.