Patents
US 8,328,960 B2#38190324 Most CitedActiveUnited States (USPTO)Utility

High strength bainitic steel for OCTG applications

2Forward Citations (#38190324 Global)
0.1/yrCitation Velocity (#39694143 Global)
1.07Citation PageRank (#38076789 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A high strength bainitic steel and a process for producing seamless pipes for OCTG applications are described. In particular, the advantages ensuing to the steel of the invention are the improvement in strength-toughness over tempered martensitic steels, and a simplified thermal treatment. Quenching is not necessary and by avoiding the quenching treatment the microstructure results far more homogeneous, which allows thick walled tubes to be produced. For the same steel composition, in comparison to conventional tempered martensitic structures, a better combination of strength and toughness can be achieved, in particular by tempering as rolled carbide-free bainitic structures.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Process A method for the production of high strength bainitic steel seamless pipes comprising the following steps: a) providing a steel having a composition comprising 0.2-0.4% by weight of C 0.05-1.5% by weight of Mn; 1.0-2.0% by weight of Si and 0-0.5% by weight of Al or, alternatively, 1.0-2.0% by weight of Al and 0-0.5% by weight of Si; 0.5-2.0% by weight of Cr; 0.2-0.5% by weight of Mo; 2.0-3.7% by weight of Ni; the remainder being iron and inevitable impurities; b) hot rolling said steel at a temperature to obtain a seamless steel pipe; c) continuously cooling the steel from the rolling

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,655,465 AHeat treatment for alloys particularly steels to be used in sour well service197238
US 3,810,793 AProcess of manufacturing a reinforcing bar steel for prestressed concrete197451
US 3,915,697 ABainitic steel resistant to hydrogen embrittlement197538
US 4,231,555 ABar-shaped torsion spring198070
US 4,336,081 AProcess of preparing steel coil spring198255
US 4,376,528 ASteel pipe hardening apparatus198356
US 4,379,482 APrevention of cracking of continuously cast steel slabs containing boron198333
US 4,407,681 AHigh tensile steel and process for producing the same198359
EP 0,092,815 A2A car stabilizer and a manufacturing method therefor—29
EP 0,102,794 A2A one piece flexible coupling—3
JP S6025719 AMethod of molding sandwich—9
JP S6086209 AManufacture of steel having high resistance against crack by sulfide—14
US 4,526,628 AMethod of manufacturing a car stabilizer198562
JP S61270355 AHigh strength steel excelling in resistance to delayed fracture—19
JP S634047 AHigh-tensile steel for oil well excellent in sulfide cracking resistance—11
JP S634046 AHigh-tensile steel for oil well excellent in resistance to sulfide cracking—8
US 4,721,536 AMethod for making steel tubes or pipes of increased acidic gas resistance198842
JP S63230847 ALow-alloy steel for oil well pipe excellent in corrosion resistance—10
JP S63230851 ALow-alloy steel for oil well pipe excellent in corrosion resistance—13
US 4,814,141 AHigh toughness, ultra-high strength steel having an excellent stress corrosion cracking resistance with a yield stress of not less than 110 kgf/mm2198938
JP H01259125 AManufacture of high-strength oil well tube excellent in corrosion resistance—10
JP H01259124 AManufacture of high-strength oil well tube excellent in corrosion resistance—8
JP H01283322 AProduction of high-strength oil well pipe having excellent corrosion resistance—11
JP H036329 AMethod for hardening steel pipe—6
JP H0421718 AProduction of high strength steel excellent in sulfide stress cracking resistance—7
JP H04107214 AInline softening treatment for air-hardening seamless steel tube—10
JP H04231414 AProduction of highly corrosion resistant oil well pipe—7
JP H0598350 AProduction of line pipe material having high strength and low yield ratio for low temperature use—13

Non-Patent Literature (5)

  • "Seamless Steel Tubes for Pressure Purposes-Technical Delivery Conditions-Part 1: Non-alloy Steel Tubes with Specified Room Temperature Properties" British Standard BS EN 10216-1:2002 E:1-26, published May 2002.
  • "Seamless Steel Tubes for Pressure Purposes-Technical Delivery Conditions-Part 2: Non-alloy and Alloy Steel Tubes with Specified Elevated Temperature Properties" British Standard BS EN 10216-2:2002+A2:2007:E:1-45, published Aug. 2007.
  • "Seamless Steel Tubes for Pressure Purposes-Technical Delivery Conditions-Part 3: Alloy Fine Grain Steel Tubes" British Standard BS EN 10216-3:2002 +A1:2004 E:1-34, published Mar. 2004.
  • "Seamless Steel Tubes for Pressure Purposes-Technical Delivery Conditions-Part 4: Non-alloy and Alloy Steel Tubes with Specified Low Temperature Properties" British Standard BS EN 10216-4:2002 + A1:2004 E:1-30, published Mar. 2004.
  • Aggarwal, R. K., et al.: "Qualification of Solutions for Improving Fatigue Life at SCR Touch Down Zone", Deep Offshore Technology Conference, Nov. 8-10, 2005, Vitoria, Espirito Santo, Brazil, in 12 pages.