Spring steel and spring having superior corrosion fatigue strength
Abstract
The present application provides a high strength spring steel and a high strength spring that have superior corrosion fatigue strength. The spring steel comprises, in terms of percent by mass, 0.35-0.55% C, 1.60-3.00% Si, 0.20-1.50% Mn, 0.10-1.50% Cr and at least one element selected from 0.40-3.00% Ni, 0.05-0.50% Mo 0.05-0.50% V, the balance being at least substantially Fe and incidental elements and impurities.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 45 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A steel alloy comprising, in terms of percent by mass: 0.47-0.49% C,
- Claim 2Depends on #1
The steel alloy according to claim 1 , wherein the following formula (3) is satisfied: 159C(%)−Si(%)+8Mn(%)+12Cr(%)≦84% (3).
- Claim 3Depends on #2
The steel alloy according to claim 2 , wherein formula (3) is less than or equal to 82%.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (45)
Non-Patent Literature (3)
- Amendment and Response to non-final Office Action mailed Apr. 25, 2012 for U.S. Appl. No. 12/892,445.
- Excerpt from the textbook SPRING, 4th edition edited by the Japan Society of Spring Engineers 2008, p. 508.
- Office Action mailed Apr. 25, 2012 for U.S. Appl. No. 12/892,445.