Patents
US 8,323,604 B2#46020128 Most CitedActiveUnited States (USPTO)Utility

Cerium salt, producing method thereof, cerium oxide and cerium based polishing slurry

1Forward Citations (#46020128 Global)
0.1/yrCitation Velocity (#50084098 Global)
1.32Citation PageRank (#28028812 Global)
20Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A cerium salt wherein, when 20 g of the cerium salt is dissolved in a mixed liquid of 12.5 g of 6N nitric acid and 12.5 g of a 30% hydrogen peroxide aqueous solution, a concentration of an insoluble component present in the solution is 5 ppm or less by mass ratio to the cerium salt before dissolution and cerium oxide produced by processing the cerium salt at high temperatures. Scratch on a surface to be polished can be reduced when a cerium based polishing slurry containing the cerium oxide particles is used, since an amount of impurities in cerium oxide particles and cerium salt particles, raw material thereof, is reduced for high purification.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A producing method of a cerium based polishing slurry, which comprises preparing a cerium salt, dissolving the cerium salt in 6N nitric acid to obtain a solution, separating and removing an insoluble component in the solution, adding a precipitating agent to obtain a precipitate of a purified cerium salt after said removing, and oxidizing the purified cerium salt to obtain cerium oxide.

  2. Claim 2Depends on #1

    The producing method of a cerium based polishing slurry according to claim 1 , wherein said separating and removing is executed so that when 20 g of the cerium salt is dissolved in a mixed liquid of 12.5 g of 6N nitric acid and 12.5 g of a 30% hydrogen peroxide aqueous solution, a concentration of an insoluble component present in the solution is 5 ppm or less by mass ratio.

  3. Claim 3Independent Claim

    The producing method of a cerium based polishing slurry according to c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
JP S5395900 AProduction of fine rare earth elements carbonate powder—3
JP H07144915 AProduction of cerium carbonate and cerium oxide—10
JP H08153696 AAbrasive and polishing—26
JP H09183966 AProduction of cerium abrasive—19
US 5,772,780 APolishing agent and polishing method199863
JP H1112561 AAbrasive for semiconductor and production of the same—27
JP 2000026840 AAbrasive—15
US 6,043,155 APolishing agent and polishing method200055
WO 0,037,578 A1Cerium oxide slurry for polishing, process for preparing the slurry, and process for polishing with the slurry—5
US 6,120,571 APolishing agent for semiconductor and method for its production200055
JP 2001089748 AAbrasive—17
JP 2001189291 ACerium oxide polishing agent, semiconductor chip, their manufacturing method, and method for polishing board—7
US 6,420,269 B2Cerium oxide abrasive for polishing insulating films formed on substrate and methods for using the same200294
JP 2002220229 AMethod for producing ammonium cerium (iv) nitrate—8
US 6,478,836 B1Cerium oxide slurry for polishing, process for preparing the slurry, and process for polishing with the slurry200237
JP 2002371267 AMethod for manufacturing cerium-containing abrasive particle and cerium-containing abrasive particle—19
JP 2003105326 ARaw material for cerium polishing material and method for analyzing raw material for cerium polishing material—9
US 6,602,111 B1Abrasive200324
JP 2003252622 AProduction method for nano acicular ceria powder—16
JP 3,510,850 B2ダブルポンプ20042

Non-Patent Literature (5)

  • Chinese Office Action dated Oct. 9, 2009, issued in corresponding Chinese Patent Application No. 2004800257778.
  • Chinese Office Action dated Sep. 21, 2011, issued in corresponding Chinese Patent Application No. 201010238216.3.
  • G. F. Smith et al.; "Hexanitrato Ammonium Cerate as a Proposed Reference Standard in Oxidimetry"; Industrial and Engineering Chemistry, Nov. 15, 1936, pp. 449-451, vol. 8, No. 6.
  • International Search Report of PCT/JP2004/013118, mailing date of Dec. 21, 2004.
  • Japanese Office Action dated Feb. 24, 2009, issued in corresponding Japanese Patent Application No. 2005-513887.