Method of manufacturing an environmentally resilient structural panel
Abstract
An environmentally resilient building product of a vinyl laminated formed-sheet metallic substrate wherein the vinyl laminate is adhesively attached to the formed-sheet metallic substrate to provide a durable and attractive surface. Possible decorative and resilient surfaces include, but are not limited to solid colors, metallic finishes, and graphical images or patterns, all available in a variety of textures.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 47 · Forward citations: 0.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for providing a decorative, environmentally resilient, structurally significant panel, comprising the steps of: providing a coiled flat, metallic sheet; unrolling the coiled metallic sheet; permanently bonding a first side of a vinyl laminate sheet material having a thickness of at least 0.0005 inches to a first side of the uncoiled flat metallic sheet being coated wherein a second side of the metallic sheet is uncoated; deforming the flat metallic sheet, with the vinyl laminate sheet material bonded thereto, to create a deformation in the metallic sheet and in the vinyl laminate shee
- Claim 2Depends on #1
The method of claim 1 , wherein the second side of the vinyl laminate sheet material comprises a graphical appearance.
- Claim 3Depends on #2
The method of claim 2 , wherein the gr
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (47)
Non-Patent Literature (5)
- "Nickeloid Seventy-Five, 1898-1973," published by American Nickeloid Company as 75th Anniversary booklet in 1973, 3 pages.
- Advertisement: "Design with the Rich Warmth of Wood Without ever Touching a Tree," by American Nickeloid Company, Appliance, Oct. 1992, 2 pages.
- Web site pages www.cladrex.com, "Clad Rex We Start with your finish," 2 pages, copyrighted by Clad-Rex, Inc., 2004.
- Web site pages www.cladrex.com/designer-coated-metals, "Clad Rex We start with your finish," 2 pages, copyrighted by Clad-Rex, Inc., 2004.
- Web site pages www.cladrex.com/designer—coated—metals, "Clad Rex We start with your finish," 2 pages, copyrighted by Clad-Rex, Inc., 2004.