Patents
US 8,313,593 B2#22327177 Most CitedActiveUnited States (USPTO)Utility

Method of heat treating a Ni-based superalloy article and article made thereby

5Forward Citations (#22327177 Global)
0.4/yrCitation Velocity (#22185341 Global)
1.18Citation PageRank (#33203830 Global)
45Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of heat treating an Ni-base superalloy article is disclosed. The method includes hot-working an article comprising an NiCrMoNbTi superalloy comprising, in weight percent, at least about 55 Ni to produce a hot-worked microstructure; solution treating the article at a temperature of about 1600° F. to about 1750° F. for about 1 to about 12 hours to form a partially recrystallized warm-worked microstructure; and cooling the article. The method also includes precipitation aging the article at a first precipitation aging temperature of about 1300° F. to about 1400° F. for a first duration of about 4 hours to about 12 hours; cooling the article to a second precipitation aging temperature; precipitation aging the article at a second precipitation aging temperature of about 1150° F. to about 1200° F. for a second duration of about 4 hours to about 12 hours; and cooling the article from the second precipitation aging temperature to an ambient temperature.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 45 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An NiCrMoNbTi superalloy article having a partially-recrystallized, warm-worked microstructure and comprising, in weight percent, about 55.0-63.0% Ni, about 19.0-22.5% Cr, about 6.5-9.5% Mo, about 2.75-4.5% Nb, about 1.0-2.3% Ti, up to about 0.35% Al, up to about 0.35% Mn, up to about 0.20% Si, up to about 0.010% S, up to about 0.20% C and up to about 0.015% P, with the balance Fe and incidental or trace impurities.

  2. Claim 2Depends on #1

    The article of claim 1 , wherein the alloy composition further comprises, in weight percent: up to about 0.05 V, up to about 0.05 Ta, up to about 1.0 Co or up to about 0.02 B, or a combination thereof.

  3. Claim 3Depends on #1

    The article of claim 1 , wherein C, Ti and Nb in any combination act as hardening constituents, and wherein, in weight percent, C is about 0.007 to about 0.011, Ti is about 1.33 to about 1.92, Nb is about 3.47 to about 4.07 and

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (45)

PatentTitleYearCitations
US 3,046,108 AAge-hardenable nickel alloy1962103
US 3,160,500 AMatrix-stiffened alloy196444
US 3,420,660 AHigh strength precipitation hardening heat resisting alloys196932
US 3,826,649 ANickel-chromium-iron alloy19748
US 3,871,928 AHeat treatment of nickel alloys197568
US 3,972,752 AAlloys having a nickel-iron-chromium base for structural hardening by thermal treatment197632
US 4,388,124 ACyclic oxidation-hot corrosion resistant nickel-base superalloys198350
US 4,400,211 AAlloy for making high strength deep well casing and tubing having improved resistance to stress-corrosion cracking198368
US 4,400,210 AAlloy for making high strength deep well casing and tubing having improved resistance to stress-corrosion cracking198349
US 4,608,094 AMethod of producing turbine disks198654
US 4,652,315 APrecipitation-hardening nickel-base alloy and method of producing same198747
EP 0,247,577 A1Corrosion resistant age hardenable nickel-base alloy—24
US 4,750,950 AHeat treated alloy198817
US 4,788,036 ACorrosion resistant high-strength nickel-base alloy198858
US 4,894,089 ANickel base superalloys199020
US 4,979,995 AMember made of nickel base alloy having high resistance to stress corrosion cracking and method of producing same199030
US 4,983,233 AFatigue crack resistant nickel base superalloys and product formed199114
US 5,059,257 AHeat treatment of precipitation hardenable nickel and nickel-iron alloys199147
US 5,124,123 AFatigue crack resistant astroloy type nickel base superalloys and product formed199214
US 5,129,970 AMethod of forming fatigue crack resistant nickel base superalloys and product formed199219
US 5,129,971 AFatigue crack resistant waspoloy nickel base superalloys and product formed199213
US 5,130,086 AFatigue crack resistant nickel base superalloys199213
US 5,130,088 AFatigue crack resistant nickel base superalloys199214
US 5,130,087 AFatigue crack resistant nickel base superalloys199213
US 5,130,089 AFatigue crack resistant nickel base superalloy199218

Non-Patent Literature (2)

  • Karl A. Heck, "The Time-Temperature-Transformation Behavior of Alloy 706", The Minerals, Metals & Materials Society, 1994, pp. 393-404.
  • Sarwan Mannan and Frank Veltry, "Time-Temperature-Transformation Diagram of Alloy 725", The Minerals, Metals & Materials Society, 2001, pp. 345-350.