System and method for conditioning and detection of susceptibility to moisture damage in asphalt mixes
Abstract
An apparatus and method for determination of susceptibility of asphalt concrete materials to moisture damage. An asphalt sample of known bulk specific gravity (density) is placed inside a chamber filled with water, which is capable of heating the sample to a predetermined temperature. The chamber is pressurized by introduction of air pressure to a flexible membrane that decreases the volume within a chamber containing the sample and water, increasing the pore pressure in the sample. The pressure is then released and allowed to come to ambient pressure. This process is repeated a predetermined number of times (cycles). When a selected number of cycles are complete, the asphalt sample is removed from the chamber and its bulk specific gravity (density) measured again. The difference between the density before and after conditioning is an excellent method of rating the degree at which moisture would deteriorate asphalt samples due to introduction of moisture. The cyclic nature of the increased/decreased pore pressure is observed to significantly decrease bulk specific gravity (density) for poor quality asphalt designs. Furthermore, the sample conditioned by this method can be used for
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 1.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for determining the susceptibility of a compacted asphalt sample to moisture damage, comprising: measuring a first density of a compacted asphalt sample; placing the compacted asphalt sample in a chamber; adding water to the chamber containing the compacted asphalt sample; sealably closing the chamber; cyclically applying pressure to the water in the closed chamber with the compacted asphalt sample therein; then measuring a second density of the compacted asphalt sample; calculating a percent difference between the first and second densities of the compacted asphalt sample; and determ
- Claim 2Depends on #1
The method of claim 1 , wherein determining whether the compacted asphalt sample is susceptible to moisture damage based on the calcula
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| CN 106,052,752 A | Hydraulic crushing device fiber rod and work plane contact tester | — | 0 |
References Cited — Backward Prior Art (11)
Non-Patent Literature (5)
- A test Method for Identifying Moisture Susceptible Asphalt Concrete Mixes, Alam et al, Center for Highway Materials Research, University of Texas at El Paso (1998).
- AASHTO Designation T283-89 "Resistance of Compacted Bituminous Mixture to Moisture Induced Damage" (1989).
- ASTM Designation D4867/D 4867M-96 "Standard Test Method for Effect of Moisture on Asphalt Concrete Paving Mixtures" (1996).
- Development and Evaluation of Test Methods to Evaluate Water Damage and Effectiveness of Antistripping Agents, Birgisson et al, Final Report Florida Dept. of Transportation (2005).
- Testing for Debonding Asphalt from Aggregates, R.A. Jimenez Transportation Research Record (1974).