Patents
US 8,308,932 B2#44313629 Most CitedActiveUnited States (USPTO)Utility

Method of recovering valuable metals from IZO scrap

2Forward Citations (#44313629 Global)
0.1/yrCitation Velocity (#39954534 Global)
0.91Citation PageRank (#47221213 Global)
44Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Provided are a method of recovering valuable metals from IZO scrap, wherein indium and zinc are recovered as hydroxides by using an IZO scrap as both an anode and a cathode, and performing electrolysis while periodically reversing polarity; and a method of recovering valuable metals from IZO scrap, wherein the hydroxides of indium and zinc obtained by the electrolysis are roasted and indium and zinc are recovered as oxides. Specifically, provided is a method which enables the efficient recovery of indium and zinc from IZO scrap such as a spent indium-zinc oxide (IZO) sputtering target and IZO mill ends arising during the manufacture of such a sputtering target.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 44 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of recovering valuable metals from IZO scrap, wherein indium and zinc are recovered as hydroxides by using an IZO scrap as both an anode and a cathode, and performing electrolysis while periodically reversing polarity.

  2. Claim 2Depends on #1

    The method of recovering valuable metals from IZO scrap according to claim 1 , wherein the hydroxides of indium and zinc obtained by the electrolysis are roasted and indium and zinc are recovered as oxides.

  3. Claim 3Depends on #2

    The method of recovering valuable metals from IZO scrap according to claim 2 , wherein the hydroxides of indium and zinc obtained by the electrolysis are subject to acid leaching to obtain a solution of indium and zinc, zinc is eliminated from the solution, and indium is further recovered by electrolysis.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (44)

PatentTitleYearCitations
US 2,915,444 AProcess for cleaning and plating ferrous metals195946
US 3,257,299 AComposition and method for electrolytic stripping of coatings from metals196616
US 4,330,377 AElectrolytic process for the production of tin and tin products198249
JP H01219186 AMethod for refining indium—7
US 4,950,326 AProcess for removal of dissolved copper from solution199019
US 4,981,564 AAdditives for electroplating compositions and methods for their use199121
JP H05156381 AMethod for recovering raw indium for electrolysis—17
US 5,290,412 AApparatus for separating electrodeposited metal in electrolytic refining199427
US 5,417,816 AProcess for preparation of indium oxide-tin oxide powder199548
JP H07145432 ARecovering method of indium—29
US 5,543,031 AMethod for recovering indium by electrowinning and apparatus therefor199620
US 5,849,221 ARaw material for producing powder of indium-tin oxide aciculae and method of producing the raw material, powder of indium-tin oxide aciculae and method of producing the powder, electroconductive paste and light-transmitting electroconductive film199813
JP H11343590 AManufacture of high purity tin—32
US 6,117,209 AHydrometallurgical process for treating alloys and drosses to recover the metal components200020
JP 2003247089 AMethod of recovering indium—53
US 6,896,788 B2Method of producing a higher-purity metal200546
JP 2005314786 AMethod for collecting indium—22
US 7,157,024 B2Metal oxide particle and process for producing same200722
JP 2007131953 AMethod for recovering indium—8
WO 2008/053616 A1Method for collection of valuable metal from ito scrap—4
WO 2008/053620 A1Method for collection of valuable metal from ito scrap—3
WO 2008/053617 A1Method for collection of valuable metal from ito scrap—3
WO 2008/053618 A1Method for collection of valuable metal from ito scrap—10
WO 2008/053619 A1Method for collection of valuable metal from ito scrap—3
WO 2008/099774 A1Method of recovering valuable metal from scrap containing conductive oxide—9
WO 2008/099773 A1Methods of recovering valuable metal from scrap containing electrically conductive oxide—8
WO 2008/117649 A1Method of recovering valuable metal from scrap containing conductive oxide—5
US 7,435,325 B2Method for producing high purity nickle, high purity nickle, sputtering target comprising the high purity nickel, and thin film formed by using said spattering target200844

Non-Patent Literature (5)

  • One page English language Abstract of JP 03-082720 A, Apr. 8, 1991.
  • One page English language Abstract of JP 08-041560 A, Feb. 13, 1996.
  • One page English language Abstract of JP 2000-169991 A, Jun. 20, 2000.
  • One page English language Abstract of JP 2002-069544 A, Mar. 8, 2002.
  • One page English language Abstract of JP 2002-069684 A, Mar. 8, 2002.